Vaporization of Strontium Atom and Ion from Strontium Oxide Applied on Tungsten and Rhenium

Mitsuru Asano, Kenji Kubo, Saburō MagariShitsuryou 1968 · DOI

Abstract

A Langmuir method has been used to determine the vapor pressure and the heats of vaporization of strontium atoms from strontium oxide applied on tungsten and rhenium surfaces. The data obtained are $\log P_{\text{atm}} = 5.064 - 2.071 \times 10^4/T$ and $l^T_0 = 4.11 \pm 0.14 \text{ eV}$ for tungsten, and $\log P_{\text{atm}} = 6.095 - 2.496 \times 10^4/T$ and $l^T_0 = 4.95 \pm 0.14 \text{ eV}$ for rhenium. By measuring the ion current of $^{88}\text{Sr}^+$ with a mass spectrometer, the heats of vaporization of strontium ions were determined as $l^T_+ = 7.07 \pm 0.08 \text{ eV}$ for tungsten and $l^T_+ = 6.73 \pm 0.07 \text{ eV}$ for rhenium, assuming the process follows the Saha-Langmuir equation. The work functions of these composite surfaces were also evaluated.

Introduction

In the mid-20th century, the thermionic and surface ionization properties of metallic oxides were critical for developing vacuum tubes and ion sources. However, experimental data for strontium oxide (SrO) was inconsistent, with reported heats of vaporization for strontium varying from 2.60 eV to 6.25 eV. These discrepancies arose from uncertainties regarding the vaporizing species (SrO molecules vs. Sr atoms) and the chemical interactions between the oxide and the underlying metal substrate. This study aims to provide definitive values by measuring both neutral atoms and positive ions while accounting for the chemical reactions at the interface.

Methodology

The researchers employed a dual-track experimental approach to capture both neutral and ionic vaporization dynamics:

  1. Neutral Atom Vaporization (Langmuir Method): Strontium nitrate was applied to tungsten (W) and rhenium (Re) ribbon filaments and thermally decomposed into SrO. Filaments were heated in a vacuum, and the mass loss was determined via EDTA titration of the remaining strontium. This allowed for the calculation of vapor pressure and the heat of vaporization ($l^T_0$).
  2. Ion Vaporization (Mass Spectrometry): A single-focusing mass spectrometer measured the $^{88}\text{Sr}^+$ ion current emitted from the heated filaments.
  3. Thermodynamic Energy Cycle: To cross-validate the data, the authors utilized a thermodynamic cycle (Figure 1) relating the heats of vaporization for atoms ($l^T_0$) and ions ($l^T_+$) to the surface work function ($\phi$) and the ionization potential ($I$) of the atom.
Figure 1: Thermodynamic cycle relating atom and ion vaporization energies to the surface work function.

Key Insights and Results

The study revealed that the metal substrate fundamentally dictates the surface chemistry. Tungsten reacts with SrO to form strontium tungstate ($SrWO_3$), releasing Sr gas, whereas rhenium is more chemically inert.

A significant finding was the quantification of work function modification. While clean tungsten has a work function of ~4.5 eV, the SrO-coated tungsten dropped to ~2.73 eV, explaining its high efficiency for thermionic emission. The final thermochemical constants derived for both substrates are summarized in Figure 2.

Figure 2: Summary of heats of vaporization and calculated work functions for SrO on tungsten and rhenium.

Discussion and Limitations

The results for tungsten align well with previous work by Wohler and Rossini, correcting earlier studies that failed to identify the specific vaporizing species. However, the study acknowledges certain limitations:

  • Vaporization Coefficient: The calculations assume a coefficient of unity, which is an idealization in the Langmuir method.
  • Surface Heterogeneity: The "patch effect" suggests that ion and electron emission may occur at different surface sites with varying local work functions. The reported $\phi$ values represent an effective average.
  • Temperature Measurement: While optical pyrometry was the standard in 1968, it introduces inherent uncertainties compared to modern techniques.

Future research into the patchy nature of these surfaces is suggested to fully reconcile the differences between ion and electron emission data.

Summary updated

Abstract

A Langmuir method has been used to determine the vapor pressure and the heats of vaporization of strontium atoms from strontium oxide applied on tungsten and rhenium surfaces. The data obtained are log Patm=5.064-2.071×104/T and lTo=4.11±0.14eV for tungsten, and log Patm=6.095-2.496×104/T and lTo=4.95±0.14eV for rhenium, respectively. By measuring the ion current of 88Sr+ with a mass spectrometer the values of the heats of vaporization of strontium ions have also been obtained as lT+=7.07±0.08eV and lT+=6.73±0.07eV for tungsten and rhenium, respectively, under the assumption that the ion vaporization processes may be described by the, Saha-Langmuir equation. The work functions of the surfaces applied with strontium oxide have been discussed.
BibTeX
@inproceedings{asano1968vaporization,
  author = {Mitsuru Asano and Kenji Kubo and Saburō Magari},
  title = {{Vaporization of Strontium Atom and Ion from Strontium Oxide Applied on Tungsten and Rhenium}},
  booktitle = {Shitsuryou},
  year = {1968},
  doi = {10.5702/massspec1953.16.315},
}
Figure