Synthesis of Precipitated Calcium carbonate in Ca(OH)2-CO2-H2O System by the Continuous Drop Method of Ca(OH)2Slurry

Ji‐Whan Ahn, Jaesung Lee, Sung-Min Joo, Hyunjung Kim, Jong‐Kuk Kim, Choon Han, Hwan Kim, Ahn, Ji-Whan, Lee, Jae-Sung, Joo, Sung-Min, Kim, Hyung-Seok, Kim, Jong-Kuk, Han, Choon, Kim, HwanJournal of the Korean Ceramic Society 2002 · DOI

Abstract

This study investigates the synthesis of Precipitated Calcium Carbonate (PCC) using a continuous drop method, where a Ca(OH)₂ slurry is introduced into a CO₂-saturated aqueous environment. The research demonstrates that the morphology and particle size of the resulting calcite crystals are governed by the balance between the CO₂ absorption rate and the Ca(OH)₂ dissolution rate. By adjusting parameters such as CO₂ flow rate and slurry concentration, the morphology can be tuned from rhombohedral (1.0 µm) to prismatic (0.1 µm) and eventually to hexagonal plate-shaped structures (0.1 µm thickness, 1.0 µm width). Under optimized conditions of 4.0 wt% slurry and 500 mL/min CO₂ flow, the system consistently produces uniform hexagonal plates.

Introduction

Precipitated Calcium Carbonate (PCC) is a critical industrial material, serving as a high-performance filler in paper, plastics, and coatings to enhance properties like whiteness, opacity, and mechanical strength. The efficacy of PCC in these applications is highly dependent on its specific crystal morphology and particle size.

Traditional synthesis methods, such as bubbling CO₂ gas directly into a bulk Ca(OH)₂ slurry, often lack the precision required to produce highly uniform or specialized crystal shapes. This paper explores the "continuous drop method" as a controllable alternative to better understand the kinetic factors—specifically the competition between gas absorption and solid dissolution—that dictate crystal growth in the Ca(OH)₂-CO₂-H₂O system.

Methodology

The experimental setup involved dropping a Ca(OH)₂ slurry (concentrations ranging from 1.0 to 4.0 wt%) at a controlled rate (60–120 drops/min) into 150 mL of distilled water. Simultaneously, CO₂ gas was introduced at flow rates ranging from 100 to 500 mL/min. The reaction progress was monitored in real-time using pH and electrical conductivity meters to track the transition from slurry to synthesized powder.

Flowchart of the continuous drop synthesis process

The resulting powders were filtered, dried, and characterized using X-ray Diffraction (XRD) for phase identification, Scanning Electron Microscopy (SEM) for morphological analysis, and Thermal Analysis (TG-DTA) to confirm chemical purity.

Results and Discussion

The study identified that the final crystal shape is a product of kinetic competition. When the CO₂ absorption rate exceeds the Ca(OH)₂ dissolution rate (typically at high gas flow and low slurry concentration), the system favors the growth of existing crystal planes, resulting in larger (~1.0 µm) rhombohedral calcite. Conversely, when dissolution exceeds absorption (low gas flow, high slurry concentration), rapid supersaturation triggers the formation of new nuclei, leading to smaller (~0.1 µm) prismatic calcite.

SEM images showing morphological variations (a-d) of synthesized PCC under different reaction conditions

Key morphological findings include:

  • Rhombohedral Calcite: Achieved at 1.0 wt% slurry and high CO₂ flow rates, yielding particles approximately 1.0 µm in size.
  • Prismatic Calcite: Synthesized when the feeding rate of the slurry exceeded the system's CO₂ absorption capacity, producing fine 0.1 µm particles.
  • Plate-shaped Calcite: By maintaining a high CO₂ flow (500 mL/min) and high stirring speed (using a 5.0 cm magnetic bar), the researchers produced hexagonal plates. At 4.0 wt% Ca(OH)₂ slurry, these plates were remarkably uniform, with a thickness of 0.1 µm and a width of 1.0 µm. This morphology arises because the (110) plane grows faster than the (001) plane under specific low-saturation conditions.

Furthermore, the study identified distinct electrical conductivity signatures for different morphologies, providing a potential method for in-situ process control in industrial settings.

Conclusion

The continuous drop method provides a robust framework for controlling PCC morphology through kinetic balancing. While effective at the laboratory scale, future research should address the engineering challenges of industrial scale-up and the potential influence of temperature variations and chemical additives on crystal growth. The ability to produce uniform hexagonal plates offers significant potential for high-performance industrial applications where specific particle geometry is paramount.

Summary updated

Abstract

Experiments were conducted to investigate the synthesis characteristics of Precipitated Calcium Carbonate(for short PCC) in Ca(OH)₂-CO₂-H₂O system by the continuous drop method of Ca(OH)₂ slurry into the solution containing CO₂(aq). When the flow rate of CO₂(g) increases and the concentration of Ca(OH)₂ slurry become low, the absorption rate of CO₂(g) become faster than the dissolution rate of Ca(OH)₂. Consequently, the growth of the calcite crystal plane is facilitated resulting in synthesis of 1.0㎛ of rhombohedral calcite. On the other hand, when the flow rate of CO₂(g) decreases and the concentration of Ca(OH)₂ slurry become high, new nuclei is created along with the crystal growth resulting in synthesis of 0.1 ㎛ of prismatic calcite. Maintaining 1.0wt% of Ca(OH)₂ slurry, 120 drops/min of drop rate and 25℃ of temperature, the shape of PCC shows colloidal and spherical agglomerate at 100 mL/min of the flow rate of CO₂(g); the mixture of rhombohedral and plate-shaped calcite, at 200∼500 mL/min. Therefore, as the flow rate of CO₂(g) increases, the shape of PCC changes from colloidal and rhombohedral calcite to plate-shaped calcite. Maintaining 500 mL/min of the flow rate of CO₂(g), 120 drops/min of the drop rate of Ca(OH)₂ slurry, and 25℃ of temperature, the shape of PCC shows the plate-shaped calcite at 1.0∼3.0 wt% of Ca(OH)₂ slurry; the hexagonal plate-shape calcite of the thickness of 0.1㎛ and the width of 1.0㎛, at 4.0 wt%.
BibTeX
@article{ahn2002synthesis,
  author = {Ji‐Whan Ahn and Jaesung Lee and Sung-Min Joo and Hyunjung Kim and Jong‐Kuk Kim and Choon Han and Hwan Kim and Ahn, Ji-Whan and Lee, Jae-Sung and Joo, Sung-Min and Kim, Hyung-Seok and Kim, Jong-Kuk and Han, Choon and Kim, Hwan},
  title = {{Synthesis of Precipitated Calcium carbonate in Ca(OH)<sub>2</sub>-CO<sub>2</sub>-H<sub>2</sub>O System by the Continuous Drop Method of Ca(OH)<sub>2</sub>Slurry}},
  journal = {Journal of the Korean Ceramic Society},
  year = {2002},
  doi = {10.4191/kcers.2002.39.4.327},
}
Figure