Abstract
Keyhole porosity is a key concern in laser powder-bed fusion (LPBF), potentially impacting component fatigue life. However, some keyhole porosity formation mechanisms, e.g., keyhole fluctuation, collapse and bubble growth and shrinkage, remain unclear. Using synchrotron X-ray imaging we reveal keyhole and bubble behaviour, quantifying their formation dynamics. The findings support the hypotheses that: (i) keyhole porosity can initiate not only in unstable, but also in the transition keyhole regimes created by high laser power-velocity conditions, causing fast radial keyhole fluctuations (2.5-10 kHz); (ii) transition regime collapse tends to occur part way up the rear-wall; and (iii) immediately after keyhole collapse, bubbles undergo rapid growth due to pressure equilibration, then shrink due to metal-vapour condensation. Concurrent with condensation, hydrogen diffusion into the bubble slows the shrinkage and stabilises the bubble size. The keyhole fluctuation and bubble evolution mechanisms revealed here may guide the development of control systems for minimising porosity.
Introduction
Laser Powder Bed Fusion (LPBF) is a cornerstone of metal additive manufacturing, yet it remains susceptible to internal defects, specifically keyhole porosity. These pores form when the high-intensity laser creates a deep, vapor-filled cavity (the keyhole) that becomes unstable and collapses, trapping gas. Such defects significantly compromise the fatigue life and structural integrity of printed components. Understanding the millisecond-scale dynamics of keyhole fluctuations and the subsequent life cycle of trapped bubbles is critical for developing defect-free manufacturing processes.
Methodology
To observe these phenomena in real-time, researchers utilized ultra-high-speed in situ synchrotron X-ray imaging at the Advanced Photon Source. This technique allowed for imaging through solid metal at 50,000 frames per second. The study focused on a high-strength aluminum alloy (Al7A77) and integrated data from previous studies on Ti-6Al-4V, Inconel 718, and stainless steel (SS304) to identify universal physical trends. Data analysis involved a custom image-processing pipeline with Kalman filters for automated bubble tracking and analytical modeling combining the Rayleigh–Plesset equation with gas diffusion theories.
Keyhole Stability and the Three-Regime Map
The research identifies three distinct keyhole regimes: quasi-stable (Regime I), transition (Regime II), and unstable (Regime III). A critical finding is the identification of the "Transition Regime," where porosity initiates not just at the bottom of the keyhole, but partway up the rear wall due to rapid radial fluctuations (2.5–10 kHz).
A universal stability metric was established using the front keyhole wall (FKW) angle (θ). When plotted against a "normalized enthalpy product," the FKW angle for various materials collapses onto a single curve. This provides a predictive "North Star" for process optimization, with critical stability thresholds identified at approximately 60° for Al7A77 and 80° for Ti-6Al-4V.
Pore Formation and Bubble Dynamics
The study reveals that pore formation in the transition regime is driven by specific rear-wall perturbations. Once a keyhole collapses and a bubble is trapped, it undergoes a three-stage life cycle: explosive growth due to pressure equalization, rapid shrinkage as metal vapor condenses, and finally, stabilization.
While metal-vapor condensation acts to eliminate the pore, hydrogen diffusion from the surrounding melt into the bubble prevents its total collapse. This diffusion "freezes" the bubble at a stable size, resulting in permanent porosity in the final part. Analytical models showed high correlation ($R^2 \approx 0.95-0.97$) with experimental data, confirming hydrogen as the primary stabilizer of these defects.
Conclusion and Future Outlook
This work provides a high-resolution map of the mechanisms governing keyhole porosity. By identifying the transition regime and the role of hydrogen in bubble stabilization, the study offers a path toward real-time monitoring and control. Future systems could potentially use acoustic signatures or optical monitoring of keyhole angles to adjust laser parameters on the fly, minimizing defects and expanding the reliability of LPBF for critical structural applications.