Synthesis and Characterization of Degradable Polymers

Christopher M. CollinsTopScholar 2019

Abstract

A degradable polymer with proposed applications in drug delivery was synthesized and characterized. This polymer was grown from a difunctional initiator, a "core" that is able to grow two polymer chains and able to degrade in the presence of oxidizing agents such as peroxides. During the first part of this project, poly(methyl methacrylate) was synthesized via atom transfer radical polymerization using commercially-available reagents in order to develop an optimal synthesis technique. This technique was then used to synthesize the degradable polymer. After introducing hydrogen peroxide, the molecular weight of the degradable polymer decreased in two different experiments, confirming its hypothesized behavior.

Introduction

Traditional degradable polymers often rely on triggers like pH changes or the presence of reducing agents. However, cancer cells are known to maintain higher-than-normal concentrations of reactive oxygen species (ROS), specifically hydrogen peroxide ($H_2O_2$). This research addresses the challenge of creating a "smart" packaging material for chemotherapy. By encapsulating drugs in a polymer that only degrades under high oxidative stress, the payload remains protected in the bloodstream (where peroxide levels are low) and is released only upon reaching the oxidative environment of a tumor, potentially reducing systemic toxicity.

Methods and Terminology

The study utilizes Atom Transfer Radical Polymerization (ATRP), a form of "living" polymerization that allows for precise control over polymer chain length and uniformity. The core innovation is a difunctional initiator (DFI) containing a boronic ester "hinge." This molecule has two active sites from which polymer chains can grow simultaneously in opposite directions.

Table of common abbreviations used in the synthesis and characterization of these polymers.

Before using the custom DFI, the reaction was optimized using a standard commercial initiator (EBiB). Different copper catalysts (CuBr vs. CuCl) and concentrations were tested to minimize the Polydispersity Index (PDI). Poly(methyl methacrylate) (PMMA) was then grown from the DFI core. The resulting polymers were analyzed using Nuclear Magnetic Resonance (NMR) to track monomer conversion and Size-Exclusion Chromatography (SEC) to measure molecular weight and PDI. Finally, purified DFI-based polymers were exposed to 100 mM hydrogen peroxide for four days to observe degradation.

Key Results and Discussion

Optimization and Growth

The transition from CuBr to CuCl and the reduction of catalyst concentration successfully lowered the PDI from 1.19 to 1.13, indicating a highly controlled, "living" reaction. Furthermore, because the DFI has two initiation sites, it was observed to grow polymer at approximately twice the rate of the monofunctional EBiB initiator, confirming that both "arms" of the molecule were active.

Oxidative Degradation

The boronic ester group acts as a chemical fuse. While stable under normal conditions, it reacts with peroxides to undergo a rearrangement that physically severs the initiator. Upon exposure to hydrogen peroxide, the DFI-based polymer showed a 58% decrease in number-average molecular weight ($M_n$), dropping from 37,700 to 15,700 daltons. This is very close to the theoretical 50% reduction expected if a chain is cut exactly in half. Following degradation, the PDI increased from 1.29 to 1.45, reflecting the transition from uniform long chains to a varied population of cleaved fragments.

Limitations and Future Outlook

While successful, some SEC data showed broad peaks, suggesting that the two chains might not always grow at identical rates. Additionally, the four-day degradation period may need to be accelerated for practical medical applications.

Future work aims to incorporate ascorbic acid (Vitamin C) pendant groups into the monomer to add antioxidant properties, potentially allowing for finer control over degradation kinetics. The author also proposes creating polymers with multiple DFI units along the backbone, allowing the material to "crumble" into many small pieces rather than just snapping in half.

Summary updated

Abstract

A degradable polymer with proposed applications in drug delivery was synthesized and characterized. This polymer was grown from a difunctional initiator, a "core" that is able to grow two polymer chains and able to degrade in the presence of oxidizing agents such as peroxides. During the first part of this project, poly(methyl methacrylate) was synthesized via atom transfer radical polymerization using commercially-available reagents in order to develop an optimal synthesis technique. This technique was then used to synthesize the degradable polymer. After introducing hydrogen peroxide, the molecular weight of the degradable polymer decreased in two different experiments, confirming its hypothesized behavior.
BibTeX
@inproceedings{collins2019synthesis,
  author = {Christopher M. Collins},
  title = {{Synthesis and Characterization of Degradable Polymers}},
  booktitle = {TopScholar},
  year = {2019},
}
Figure