Growth and Scintillation Properties of La(Cl 0.05 Br 0.95 ) 3 :Ce Crystal
Lists
Only you see this
Abstract
The growth and scintillation properties of La0.97 (Cl0.05Br0.95)3:Ce0.03 crystals are reported. A 1-inch-diameter as-grown crystal is achieved by applying the vertical Bridgman technique, and one machined single crystal with sizes 18 mm × 8 mm × 8 mm is acquired. The scintillation properties of La0.97 (Cl0.05Br0.95)3:Ce0.03 crystals are presented. Under the excitation of UV (ultraviolet) light, the crystal exhibits two luminescent peaks centered at 358 nm and 382 nm. The light output is about 62000 ph/MeV while the energy resolution (ΔE/E) of this crystal at 662 keV is 4.55% of the full width at half-maximum. Additionally, the crystal photoluminescence decay time constant is 17.7 ns, which is significantly faster than that of LaBr3:Ce. The results indicate that the LaCl3 and the LaBr3 can form the anion solid solution crystal. The Lax (ClyBr1−y)3:Cei−x crystal is potentionally a promising scintillator.
BibTeX
@inproceedings{bao2013growth,
author = {Hanbo Bao and Laishun Qin and Yanguo Ding and Zhengguo Li and Hongsheng Shi and Kangying Shu},
title = {{Growth and Scintillation Properties of La(Cl <sub>0.05</sub> Br <sub>0.95</sub> ) <sub>3</sub> :Ce Crystal}},
booktitle = {Chinese},
year = {2013},
doi = {10.1088/0256-307x/30/8/088101},
}Loading related content...