Abstract
The development of Zn-free anodes to inhibit Zn dendrite formation and modulate high-capacity Zn batteries is highly applauded yet very challenging. Here, we design a robust two-dimensional antimony/antimony-zinc alloy heterostructured interface to regulate Zn plating. Benefiting from the stronger adsorption and homogeneous electric field distribution of the Sb/Sb₂Zn₃-heterostructured interface in Zn plating, the Zn anode enables an ultrahigh areal capacity of 200 mAh cm⁻² with an overpotential of 112 mV and a Coulombic efficiency of 98.5%. An anode-free Zn-Br₂ battery using the Sb/Sb₂Zn₃-heterostructured interface@Cu anode shows an attractive energy density of 274 Wh kg⁻¹ with a practical pouch cell energy density of 62 Wh kg⁻¹. The scaled-up Zn-Br₂ battery in a capacity of 500 mAh exhibits over 400 stable cycles. Further, the Zn-Br₂ battery module in an energy of 9 Wh (6 V, 1.5 Ah) is integrated with a photovoltaic panel to demonstrate the practical renewable energy storage capabilities. Our superior anode-free Zn batteries enabled by the heterostructured interface enlighten an arena towards large-scale energy storage applications.
Introduction
Aqueous zinc (Zn) batteries are a promising alternative to lithium-ion for grid-scale storage due to their safety, low cost, and environmental sustainability. However, they face two major hurdles: dendrite growth and low energy density. During charging, zinc tends to plate unevenly, forming spiky crystals that pierce the separator and short-circuit the battery. Furthermore, most Zn batteries use a massive excess of zinc foil, which adds dead weight. The "anode-free" configuration—where zinc is plated directly from the electrolyte onto a current collector—maximizes energy density but is notoriously difficult to stabilize at high capacities.
Design and Characterization of the Heterostructured Interface
To address these challenges, a robust 2D Sb/Sb₂Zn₃ heterostructured interface (HI) was designed on a copper (Cu) current collector. Antimony (Sb) was electroplated onto Cu foil, and during initial zinc plating, the Sb reacts with Zn to form a stable Sb₂Zn₃ alloy layer.
High-resolution transmission electron microscopy (HRTEM) and energy-dispersive X-ray spectroscopy (EDS) mapping confirmed the successful formation of this interface. Density Functional Theory (DFT) calculations revealed that the Sb(104) surface has a much stronger adsorption energy for Zn atoms (-3.12 eV) compared to the Zn(100) surface (-0.72 eV), promoting uniform nucleation rather than clumping.
Electrochemical Performance and Scaling
The Sb/Sb₂Zn₃ interface significantly reduces the nucleation overpotential compared to bare Cu or Zn foil. This "zincophilic" advantage ensures a homogeneous electric field distribution, eliminating the "tip effect" that typically drives dendrite growth.
The Sb@Cu anode achieved a record-breaking stable areal capacity of 200 mAh cm⁻² with a Coulombic Efficiency (CE) of 98.5%. In full-cell tests, a Zn-Br₂ battery reached an energy density of 274 Wh kg⁻¹ (based on active materials). Practical scaling was demonstrated with a 500 mAh pouch cell maintaining stability over 400 cycles and a 9 Wh battery module successfully integrated with a photovoltaic panel to power a 10 W LED display.
Conclusion
While the 98.5% Coulombic Efficiency is a significant achievement for aqueous systems, further optimization is needed to reach the >99.9% threshold required for long-term commercial standards. Nevertheless, this heterostructured interface strategy provides a robust template for high-capacity, anode-free metal batteries, offering a clear path toward large-scale, safe renewable energy storage.