@article{ruan2022weld,
author = {Guijian Ruan and Fuqiang He and Hansen Long and Zhinan Guo and Quan Tang and Bo Tao and Shidong Li and Yongcheng Cao},
title = {{Weld defect detection of power battery pack based on image segmentation}},
journal = {International Journal of Wireless and Mobile Computing},
year = {2022},
doi = {10.1504/ijwmc.2022.10051259},