Chun-Hung Huang, Ikai Wang, Yuming Lin, Yao‐Hsuan Tseng, Chunmei LuJournal of Molecular Catalysis A Chemical 2009 · DOI

TL;DR

Researchers have developed PtOx-modified TiO2 catalysts that effectively degrade nitric oxides (NOx) under visible light. This advancement is crucial for utilizing solar energy more efficiently in air purification, overcoming the limitations of traditional UV-activated TiO2.

What Problem Does This Paper Address?

Titanium dioxide (TiO2) is a well-established photocatalyst for environmental remediation, including the degradation of nitrogen oxides (NOx). However, its effectiveness is severely limited by its wide band gap (3.2 eV), which means it can only absorb UV light, accounting for a mere 4% of the solar spectrum. The vast majority of solar energy, particularly in the visible light region (45%), remains unutilized. To address this, researchers are exploring methods to modify TiO2 to enhance its visible light absorption and photocatalytic activity. Previous attempts have involved non-metal doping or dye sensitization, but these have had their own drawbacks. This paper focuses on modifying TiO2 with platinum oxide (PtOx) to create a visible-light-responsive photocatalyst for NOx degradation.

Methods

The study employed two primary synthesis methods to create PtOx-modified TiO2 catalysts:

  • Sol-gel process: This method involved incorporating platinum precursors (Pt(NH3)4(NO3)2 or H2Pt(OH)6) directly into the TiO2 matrix during its formation. The resulting catalysts were labeled Pt2-TiO2 and Pt4-TiO2.
  • Impregnation method: In this approach, pre-synthesized TiO2 (either commercial UV100 or home-made) was loaded with platinum precursors. This method was used to create Pt2/UV100, Pt4/UV100, Pt2/TiO2, and Pt4/TiO2. A reduced platinum catalyst (Pt0/UV100) was also prepared by hydrogen reduction.

The synthesized catalysts were characterized using:

  • FE-SEM: To observe particle size and morphology.
  • XRD: To determine crystal structure.
  • Nitrogen adsorption (BET): To measure specific surface areas.
  • UV-vis spectroscopy: To analyze light absorption properties and calculate band gaps using the Kubelka-Munk theory and Tauc plots.
  • XPS: To investigate surface elemental composition and chemical states of platinum.

The photocatalytic activity was evaluated by measuring the degradation of nitric oxides (NOx) in a continuous flow reactor under various light sources (UV, blue LED, green LED, red LED) at controlled humidity and temperature. Key performance metrics included NO conversion, NO2 selectivity, and total NOx removal.

Datasets

Not discussed in the paper. The study focuses on the synthesis and characterization of novel photocatalytic materials and their performance in a controlled experimental setup.

Key Insights and Ideas

  • PtOx as a Visible Light Sensitizer: The introduction of PtOx onto TiO2 significantly enhances its activity under visible light, a crucial step towards utilizing solar energy more effectively for air purification.
  • Mixed Valence States of Platinum: XPS analysis revealed that PtOx exists in mixed valence states (PtO-PtO2) on the TiO2 surface. This mixed state is hypothesized to be key to its visible light response and ability to further oxidize NO2 to NO3-.
  • Impregnation Method Superior for Visible Light: The impregnation method, particularly with H2Pt(OH)6 as the precursor (leading to Pt4/UV100 and Pt4/TiO2), generally resulted in better visible light activity compared to the sol-gel method. This suggests that having PtOx on the TiO2 surface is more beneficial than being embedded within the matrix.
  • Precursor Choice Matters: Using H2Pt(OH)6 as the platinum precursor led to better performance than Pt(NH3)4(NO3)2. This is attributed to the latter introducing nitrate impurities that could hinder photocatalytic activity.
  • Home-made TiO2 Shows Intrinsic Visible Activity: The home-made TiO2 exhibited some visible light absorption, likely due to residual carbonate species from the sol-gel synthesis, which contributed to its better performance compared to commercial UV100.
  • Reduced NO2 Selectivity is Key: The PtOx-modified catalysts not only converted NO but also showed a reduced selectivity for NO2, indicating a more complete oxidation to NO3-. This is important as NO2 is more toxic than NO.

Key Results

  • Enhanced Visible Light Activity: PtOx-modified TiO2 catalysts, especially Pt4/UV100 and Pt4/TiO2, demonstrated significantly improved NOx degradation under visible light compared to bare TiO2.
  • Reduced NO2 Selectivity: The modified catalysts showed lower NO2 selectivity, meaning they were more effective at oxidizing NO2 to NO3-. For example, Pt4/TiO2 achieved a total NOx removal of up to 33% even under red light illumination.
  • Stable Catalyst Properties: The modification with 1% PtOx and calcination at 200°C did not significantly alter the particle size, crystal structure (anatase phase), or surface area of the TiO2.
  • PtOx on Surface is Beneficial: PtOx deposited on the TiO2 surface (via impregnation) was more effective for visible light response than PtOx doped within the TiO2 matrix (via sol-gel).
  • Pt0/UV100 for UV Activity: The Pt0/UV100 catalyst (metallic platinum) showed improved UV total NOx removal and better total oxidation of NO to NO3-, but was not effective under visible light.

Limitations and Future Work

  • Nitrate Impurities: The use of Pt(NH3)4(NO3)2 as a precursor introduced nitrate impurities, which could affect photocatalytic performance. Future work could focus on developing PtOx precursors that avoid such impurities.
  • Carbonaceous Residues: The home-made TiO2 had higher carbon content, contributing to its visible light activity. Further investigation into the role and optimization of these carbonaceous species could be beneficial.
  • Mechanism of PtOx Sensitization: While the mixed valence states of PtOx are implicated, a more detailed understanding of the exact mechanism by which they sensitize TiO2 to visible light and facilitate NOx oxidation could lead to further catalyst design improvements.
  • Long-term Stability: Although the paper mentions durability tests, long-term stability under continuous operation and varying environmental conditions would be an important area for future research.
  • Scale-up: The study was conducted at a laboratory scale. Investigating the scalability of these synthesis methods and the performance of the catalysts in larger-scale applications would be a logical next step.

Summary updated

BibTeX
@article{huang2009visible,
  author = {Chun-Hung Huang and Ikai Wang and Yuming Lin and Yao‐Hsuan Tseng and Chunmei Lu},
  title = {{Visible light photocatalytic degradation of nitric oxides on PtOx-modified TiO2 via sol–gel and impregnation method}},
  journal = {Journal of Molecular Catalysis A Chemical},
  year = {2009},
  doi = {10.1016/j.molcata.2009.10.015},
}