Ultra‐small Metallic Nickel Nanoparticles on Dealuminated Zeolite for Active and Durable Catalytic Dehydrogenation

Huixin Wu, Hai Wang, Yating Lv, Yuexin Wu, Yike Wang, Qingsong Luo, Hui Yu, Lujie Liu, Mengting Zhang, Kunming Hou, Lina Li, Jianrong Zeng, Weili Dai, Liang Wang, Feng‐Shou XiaoAngewandte 2024 · DOI

Abstract

Abstract Each step in the catalyst synthesis process plays an important role in tuning the catalyst structures. For zeolite‐supported nickel catalysts, we found the conventional calcination‐reduction method typically leads to the formation of large nickel particles, but a pre‐aging in hydrogen or nitrogen at a low temperature prior to final reduction can result in ultra‐small nickel nanoparticles in a metallic state. This pre‐aging treatment facilitates the interaction between Ni 2+ cations and silanol nests on zeolite before the decomposition of the metal salt, leading to the formation of nanoparticles with an average diameter of ~1.2 nm. In contrast, the pre‐calcination in oxygen caused the Ni 2+ aggregation before the decomposition of the metal salt precursor, yielding nickel nanoparticles larger than 5 nm. Given the structure sensitivity of nickel in cyclohexane dehydrogenation for hydrogen production, the ultra‐small nickel nanoparticles exhibited significantly enhanced activity and durability compared to previous nickel catalysts.
BibTeX
@inproceedings{wu2024ultrasmall,
  author = {Huixin Wu and Hai Wang and Yating Lv and Yuexin Wu and Yike Wang and Qingsong Luo and Hui Yu and Lujie Liu and Mengting Zhang and Kunming Hou and Lina Li and Jianrong Zeng and Weili Dai and Liang Wang and Feng‐Shou Xiao},
  title = {{Ultra‐small Metallic Nickel Nanoparticles on Dealuminated Zeolite for Active and Durable Catalytic Dehydrogenation}},
  booktitle = {Angewandte},
  year = {2024},
  doi = {10.1002/ange.202420306},
}

Loading related content...

Figure