Tribological Properties of MoN/TiN Multilayer Coatings Prepared via High-Power Impulse Magnetron Sputtering

Jiaming Xu, Ping Zhang, Jianjian Yu, Puyou Ying, Tao Yang, Jianbo Wu, Tianle Wang, N. K. Myshkin, Vladimir LevchenkoLubricants 2025 · DOI

TL;DR

This paper introduces MoN/TiN multilayer coatings fabricated using High-Power Impulse Magnetron Sputtering (HiPIMS) to overcome the limitations of single-layer nitride coatings under high loads. These novel coatings exhibit significantly improved hardness, toughness, and wear resistance, outperforming traditional TiN and MoN coatings and showing promise for extreme-load applications.

What Problem Does This Paper Address?

Transition metal nitride (TMN) coatings like TiN and MoN are widely used for their hardness and wear resistance in mechanical applications. However, monolithic TMN coatings often struggle to balance hardness with toughness, leading to premature failure under high-stress or prolonged friction conditions. This limitation hinders their use in demanding environments. While strategies like elemental doping and multilayer designs have shown promise, achieving optimal performance, especially under extreme loads, remains a challenge. This research aims to address this by developing and evaluating MoN/TiN multilayer coatings prepared via HiPIMS, a technique known for producing high-quality films with enhanced properties.

Methods

The researchers prepared MoN/TiN multilayer coatings, along with TiN and MoN monolithic coatings as controls, using High-Power Impulse Magnetron Sputtering (HiPIMS). This technique utilizes highly ionized plasmas to achieve intense ion bombardment, leading to denser and more robust films.

Key characterization techniques included:

  • Scanning Electron Microscopy (SEM): To observe the surface morphology and cross-sectional microstructure of the coatings.
  • Grazing-Incidence X-ray Diffraction (GIXRD): To analyze the phase structure and crystallographic orientation of the coatings.
  • Nanoindentation: To measure the hardness (H) and elastic modulus (E) of the coatings, and to calculate the H/E and H³/E² ratios, which are indicators of wear resistance and toughness.
  • Vickers Indentation: To assess fracture toughness (K₁c) by observing crack propagation under load.
  • Rockwell-C Hardness Indentation: To evaluate coating adhesion.
  • Reciprocating Friction and Wear Testing: To measure the coefficient of friction (COF) and wear rate under varying loads (5 N to 25 N) and sliding conditions.
  • White-light Interferometry: To analyze wear traces and determine volume loss for wear rate calculations.
  • Energy-Dispersive X-ray Spectroscopy (EDX): To map elemental distribution within the wear tracks.

Datasets

Not discussed in the paper.

Key Insights and Ideas

  • HiPIMS is Key: The use of HiPIMS is crucial for achieving the superior properties of the MoN/TiN coatings. Its ability to generate highly ionized plasma leads to better film density, reduced defects, and enhanced adhesion compared to conventional PVD methods.
  • Multilayer Architecture for Crack Suppression: The alternating MoN and TiN layers act as barriers, effectively deflecting and hindering crack propagation. This "interfacial crack-deflection" mechanism is a primary reason for the improved toughness and wear resistance.
  • Synergistic Effect of MoN and TiN: The combination of MoN and TiN in a multilayer structure appears to offer synergistic benefits. MoN contributes to COF reduction, while the multilayer design enhances overall mechanical integrity.
  • Dominant (111) Orientation: The MoN/TiN coatings exhibit a preferred (111) crystallographic orientation. This orientation is known for its high atomic packing density and lower surface energy, which directly contributes to improved hardness and wear resistance.
  • Balancing Hardness and Toughness: The MoN/TiN multilayer coatings achieve an optimal balance between hardness and toughness, a critical challenge for single-layer coatings. This balance is reflected in the high H³/E² ratio and fracture toughness values.

Key Results

  • Superior Wear Resistance: The MoN/TiN multilayer coatings demonstrated significantly better wear resistance. They maintained stable wear rates below 20 N, whereas TiN coatings failed at 5 N and MoN coatings failed at 10 N. The MoN/TiN coatings ultimately failed at 25 N, indicating a critical load capacity far exceeding the monolithic coatings.
  • Low and Stable COF: The MoN/TiN multilayer coatings exhibited a consistently low coefficient of friction (COF) of approximately 0.3–0.34, which is lower than that of TiN (~0.7–0.8) and MoN (~0.4).
  • Enhanced Hardness and Toughness: The MoN/TiN multilayer coating achieved the highest hardness (32.34 GPa), a significant improvement over TiN (19.73 GPa) and MoN (23.98 GPa). They also displayed the highest fracture toughness (K₁c = 1.64 MPa·m¹/²).
  • Improved Microstructure: SEM analysis revealed a denser, more compact microstructure with refined columnar grains in the MoN/TiN coatings, attributed to the multilayer architecture disrupting columnar growth.

Limitations and Future Work

  • Substrate Exposure at High Loads: While significantly improved, the MoN/TiN multilayer coatings still experienced substrate exposure and failure at 25 N. This indicates that while the multilayer design enhances load capacity, there's still room for further optimization for even higher extreme-load applications.
  • Future Work: The paper suggests that the MoN/TiN multilayer architecture offers a promising design for extreme-load applications. Future work could focus on further optimizing the layer thicknesses, composition, and deposition parameters to push the failure load even higher and explore their performance in specific industrial applications. Investigating the long-term durability and performance under different environmental conditions (e.g., high temperature, corrosive environments) would also be valuable.

Summary updated

Abstract

To address the limitations of single-layer nitride coatings, such as poor load adaptability and low long-term durability, MoN/TiN multilayer coatings were prepared via high-power impulse magnetron sputtering (HiPIMS). HiPIMS produces highly ionized plasmas that enable intense ion bombardment, yielding nitride films with enhanced mechanical strength, durability, and thermal stability versus conventional methods. The multilayer coating demonstrated a low coefficient of friction (COF, ~0.4) and wear rate (1.31 × 10−7 mm3/[N·m]). In contrast, both TiN and MoN coatings failed at 5 N and 10 N loads, respectively. Under increasing loads, the multilayer coating maintained stable wear rates (1.84–3.06 × 10−7 mm3/[N·m]) below 20 N, and ultimately failed at 25 N. Furthermore, the MoN layer contributes to COF reduction. Grazing-incidence X-ray diffraction analysis confirmed the enhanced crystallographic stability of the multilayer coating, thereby revealing a dominant (111) orientation. The multilayer architecture suppresses crack propagation while effectively balancing hardness and toughness, offering a promising design for extreme-load applications.
BibTeX
@inproceedings{xu2025tribological,
  author = {Jiaming Xu and Ping Zhang and Jianjian Yu and Puyou Ying and Tao Yang and Jianbo Wu and Tianle Wang and N. K. Myshkin and Vladimir Levchenko},