Thermally activated pop-in and indentation size effects in GaN films
Lists
Only you see this
Abstract
Abstract Indentation tests on epitaxial GaN thin films, grown by metalorganic chemical vapour deposition on Si (1 1 1) substrate, were conducted at temperatures of 23, 100 and 180 °C. The first pop-in events were statistically analysed with Schuh's model and resulted in thermal activation energy of 850 ± 36 meV, activation volume of 10.8 ± 1.6 Å 3 and frequency factor of 4.23 × 10 21 m −3 s −1 . In addition, the experimental results show that the critical force at the first pop-in event and the measured shear strength depend on the indenter tip radius.
BibTeX
@article{lu2012thermally,
author = {Jun-Yong Lu and Hang Ren and Dongmei Deng and Yong Wang and Kevin J. Chen and Kei May Lau and Tong‐Yi Zhang},
title = {{Thermally activated pop-in and indentation size effects in GaN films}},
journal = {Journal of Physics D Applied Physics},
year = {2012},
doi = {10.1088/0022-3727/45/8/085301},
}Loading related content...