Thermal Stability of BNCT Neutron Production Target Synthesized by In-Situ Lithium Deposition and Ion Implantation
Abstract
To testify thermal stability of the BNCT neutron target synthesized by in-situ lithium deposition and ion implantation, laser heating test of the Li3N/Li/Cu tri-layered target was conducted in high vacuum chamber of 10−6 Pa and thermal stability of the tri-layered target was characterized by X-ray photoelectron spectroscopy. Following conclusions were derived; (1) The Li3N/Li/Cu tri-layered target with very low oxide and carbon contamination was synthesized by in-situ lithium deposition and ion implantation techniques without H2O and O2 additions, (2) The starting temperature of evaporation of the Li3N/Li/Cu tri-layered target increased by 120 K compared to that of the Li/Cu target, and (3) Frequent repair synthesis of the damaged Li3N/Li/Cu tri-layered target caused by evaporation is possible.
BibTeX
@article{ishiyama2013thermal,
author = {Shintaro Ishiyama and Yuji Baba and Ryo Fujii and Masaru Nakamura and Yoshio Imahori},
title = {{Thermal Stability of BNCT Neutron Production Target Synthesized by In-Situ Lithium Deposition and Ion Implantation}},
journal = {Journal of the Japan Institute of Metals and Materials},
year = {2013},
doi = {10.2320/jinstmet.j2013048},