The Influence of Deposition Temperature on the Microscopic Process of Diamond-like Carbon (DLC) Film Deposition on a 2024 Aluminum Alloy Surface

Li Yang, Tong Li, Baihui Shang, Lili Guo, Tong Zhang, Weina HanCrystals 2024 · DOI

TL;DR

This study investigates how deposition temperature affects the formation and properties of diamond-like carbon (DLC) films on 2024 aluminum alloy. The researchers found that increasing the deposition temperature leads to thinner DLC films but also improves their adhesion to the substrate, with an optimal temperature of 100°C yielding the strongest bond. Crucially, the deposition temperature must remain below the aging temperature of the aluminum alloy to avoid degrading its properties.

What Problem Does This Paper Address?

Aluminum alloys, like the widely used 2024 alloy, are prized for their low density and high strength, making them essential in aerospace and automotive industries. However, their inherent low hardness and wear resistance limit their application in demanding environments. Surface modification techniques, such as plasma-enhanced chemical vapor deposition (PECVD) for creating diamond-like carbon (DLC) films, offer a promising solution to enhance these properties. While DLC films are known for their hardness and low friction, their performance is highly dependent on deposition parameters. Specifically, the deposition temperature is a critical factor influencing the film's microstructure, bonding with the substrate, and ultimately, its mechanical properties. This paper aims to elucidate the microscopic mechanisms by which deposition temperature impacts DLC film formation on 2024 aluminum alloy, providing crucial insights for optimizing the coating process.

Methods

The researchers employed plasma-enhanced chemical vapor deposition (PECVD) to deposit DLC films on 2024 aluminum alloy substrates. They systematically varied the deposition temperature from 50°C to 150°C. To analyze the resulting films, a suite of advanced characterization techniques was utilized:

  • Field Emission Scanning Electron Microscopy (FE-SEM) and Ultra-Depth-of-Field Microscopy: Used to observe the cross-sectional morphology of the DLC films and the scratch damage.
  • Energy-Dispersive Spectroscopy (EDS): Employed to determine the elemental distribution (C, Si, Al) within the film and at the film-substrate interface.
  • X-Ray Diffraction (XRD): Utilized to identify the phase composition of the transition layer between the DLC film and the substrate.
  • Scratch Testing (MST-4000): Performed to evaluate the adhesion strength between the DLC film and the 2024 aluminum alloy substrate. Acoustic emission signals and friction coefficients were monitored during the scratch test.

Datasets

Not discussed in the paper. The study relies on experimental samples prepared by the authors.

Key Insights and Ideas

  • The crucial role of a transition layer: A distinct transition layer containing silicon elements forms between the DLC film and the aluminum alloy substrate. This layer, identified as an aluminum-silicon solid solution, significantly enhances the bonding strength between the film and the substrate.
  • Temperature-dependent film thickness: As deposition temperature increases, the thickness of the DLC film decreases. This is attributed to changes in particle behavior within the plasma, including reduced particle density and increased residual energy per particle, leading to less efficient deposition.
  • Optimal adhesion at 100°C: The study identified 100°C as the optimal deposition temperature for achieving the maximum film-substrate bonding force (14.45 N).
  • Substrate integrity is paramount: Exceeding the aging temperature of the 2024 aluminum alloy (around 130°C) during deposition can lead to segregation of alloying elements (like copper and aluminum), negatively impacting the substrate's properties. Therefore, deposition should occur below this critical temperature.
  • Microstructural evolution: At higher temperatures (150°C), the second phase within the aluminum alloy matrix undergoes segregation, which is undesirable.

Key Results

  • Film Thickness: Decreased from 8.72 µm at 50°C to 5.37 µm at 150°C.
  • Film-Substrate Adhesion: The maximum bonding force was observed at 100°C, reaching 14.45 N. Lower temperatures (50°C) resulted in significantly weaker adhesion (4.86 N).
  • Microstructure: A silicon-containing transition layer was consistently observed. At 150°C, segregation of the aluminum alloy's second phase was noted.
  • Scratch Morphology: At 50°C, significant cracking was observed around scratches. At 100°C, cracking was reduced, and the damage was contained within the film. At 125°C and 150°C, minor detachment was observed.

Limitations and Future Work

The authors acknowledge that the deposition temperature should be kept below the aging temperature of the 2024 aluminum alloy to preserve its properties. While they identify 100°C as optimal for adhesion, further research could explore the trade-offs between film thickness, adhesion, and other critical properties like hardness and wear resistance at various temperatures. Future work could also investigate the specific mechanisms of segregation at higher temperatures and explore alternative deposition strategies or post-deposition treatments to further optimize DLC films on aluminum alloys for specific applications. The study also implicitly suggests that understanding the precise aging temperature of the specific 2024 aluminum alloy batch used would be beneficial for precise process control.

Summary updated

Abstract

In this experiment, plasma-enhanced chemical vapor deposition technology was used to deposit diamond-like carbon thin films on the surface of a 2024 aluminum alloy. The effects of deposition temperature on the microstructure, carbon, silicon, and aluminum element distribution, and film substrate adhesion of diamond-like carbon thin films were studied using field emission scanning electron microscopy, energy-dispersive spectroscopy, XRD, scratch gauge, and ultra-depth-of-field microscopy. The results showed that with the increase in deposition temperature, the thickness of DLC film decreased from 8.72 μm to 5.37 μm, and the film bonded well with the substrate. There is a clear transition layer containing silicon elements between the DLC film and the aluminum alloy substrate. The transition layer is a solid solution formed by aluminum and silicon elements, which increases the bonding strength between the film and substrate. C-Si and C-C exist in the form of covalent bonds and undergo orbital hybridization, making the DLC film more stable. When the deposition temperature exceeds the aging temperature of a 2024 aluminum alloy, it will affect the properties of the aluminum alloy substrate. Therefore, the deposition temperature should be below the aging temperature of the 2024 aluminum alloy for coating. At a deposition temperature of 100 °C, the maximum membrane substrate bonding force is 14.45 N. When a continuous sound signal appears and the friction coefficient is the same as that of the substrate, the film is completely damaged. From the super-depth map of the scratch morphology, it can be seen that, at a deposition temperature of 100 °C, a small amount of thin film detachment appears around the scratch.
BibTeX
@inproceedings{yang2024influence,
  author = {Li Yang and Tong Li and Baihui Shang and Lili Guo and Tong Zhang and Weina Han},
  title = {{The Influence of Deposition Temperature on the Microscopic Process of Diamond-like Carbon (DLC) Film Deposition on a 2024 Aluminum Alloy Surface}},
  booktitle = {Crystals},
  year = {2024},
  doi = {10.3390/cryst14110950},
}
Figure