Abstract

The present work summarizes the indentation fracture technique for the assessment of residual stresses in thin films deposited on brittle substrates by using a Vickers indenter tip. Based on a simplified analysis and experimental observations, we proposed a semi-empirical formula, i.e.,p/c<sup>3/2</sup>= K<sub>IC</sub>/χ+γ-δσ<sub>r</sub>t/c<sup>1/2</sup> to characterize film residual stresses. In the semi-empirical formula, c and p denote the crack length and the indentation load, respectively, t and r σ<sub>r</sub> are the film thickness and film stress, respectively, χ, γ, and δ are three constants, and K<sub>IC</sub> is the fracture toughness of the system and approximately equals the fracture toughness of the substrate when the crack length is much larger than the film thickness. Using the stress data from the curvature measurements, we have calibrated the dimensionless parameters introduced. δ has a value of about 59. The dimensional parameter χ changes from 0.11 to 0.145 with a mean of 0.124. The semiempirical formula introduces a physical parameter, γ, in units of N/m, to represent the nature of indentation fracture on the bare silicon wafers. The experimental results have shown that γ ranges from 1.87 to 2.52 ×10<sup>4</sup> N/m with a mean 2.26 (±0.28) ×10<sup>4</sup> N/m. Experimental results on various thin films deposited on Si wafers verify the semi-empirical formula.
BibTeX
@inproceedings{zhang2005indentation,
  author = {Tong‐Yi Zhang},
  title = {{The Indentation Fracture Technique for Measurements of Film Stresses}},
  booktitle = {Rare},
  year = {2005},
}

Loading related content...

Figure