NeurIPS 2026Coming to NeurIPS?Explore papers, orals & directions

The Corrosion Behavior of Ni-Based Superalloy Irradiated by Intense Pulsed Ion Beam

Huoping Zhong, J Zhang, Xiang Yu, Jie Shen, G. Y. Liang, Xiaojun Cui, X F Zhang, G L Zhang, Sha Yan, X.y. LeJournal of Physics Conference Series 2017

Abstract

Intense pulsed ion beam (IPIB) has been extensively used in the surface strengthening of metal materials in the past decades. Quite a lot of these materials need to be operated in the corrosive environment. Therefore, it is of significance to research the corrosion behavior of metal materials after IPIB irradiation. In this work, the corrosion behavior of Ni-based superalloy irradiated by IPIB in NaCl solution was studied. Compared to the original samples, after IPIB irradiation the corrosion resistance of samples were improved, and craters were formed on the surface of Ni-based super alloys. It is found that micro-areas with craters would be eroded prior to other areas in caustic solutions. The analysis revealed that craters play an important role in the corrosion process of the metal after irradiation. This research would help understand the influence of craters induce by IPIB on the operational performance of metal materials.
BibTeX
@article{zhong2017corrosion,
  author = {Huoping Zhong and J Zhang and Xiang Yu and Jie Shen and G. Y. Liang and Xiaojun Cui and X F Zhang and G L Zhang and Sha Yan and X.Y. Le},
  title = {{The Corrosion Behavior of Ni-Based Superalloy Irradiated by Intense Pulsed Ion Beam}},
  journal = {Journal of Physics Conference Series},
  year = {2017},
  doi = {10.1088/1742-6596/830/1/012079},
}

Loading related content...

Figure