NeurIPS 2026Coming to NeurIPS?Explore papers, orals & directions

Synthesis and properties of Pb0.92Sr0.08(Nb1-yTay)2O6 high Curie temperature piezoelectric ceramics

Wu Feng-min, Min Gao, Zhengkui Wang, Xunjun He, Bin Yang, Jiuxing JiangIntegrated 2017

Abstract

Two-step sintering process was used to prepare Pb0.92Sr0.08(Nb1-yTay)2O6(0 ≤ y ≤ 0.09) ceramics. By XRD diffraction patterns, the components were all formed orthogonal tungsten bronze structure of ferroelectric phase. Through the SEM, after doping Ta5+, the ceramic grains obviously formed a closer packed structure. With the increase of Ta5+ content, grain size decreased. The Ta5+ ions added reduced the Curie temperature, which was still higher than 530°C. Component y = 0.01 had excellent comprehensive performance, the piezoelectric constant of 79 pC/N, the Curie temperature of 562°C, the electromechanical coupling coefficient of 35.33%.
BibTeX
@inproceedings{fengmin2017synthesis,
  author = {WU Feng-min and Min Gao and Zhengkui Wang and Xunjun He and Bin Yang and Jiuxing Jiang},
  title = {{Synthesis and properties of Pb<sub>0.92</sub>Sr<sub>0.08</sub>(Nb<sub>1-y</sub>Ta<sub>y</sub>)<sub>2</sub>O<sub>6</sub> high Curie temperature piezoelectric ceramics}},
  booktitle = {Integrated},
  year = {2017},
  doi = {10.1080/10584587.2017.1352389},
}

Loading related content...

Figure