Study on the Leaching Conditions of the Shihongtan Uranium Deposit

Xin Yuan, Jinhui Liu, Lingling Xu, Yipeng Zhou, Kai Zhao, Mintao HuMetals 2023 · DOI

TL;DR

This study investigates the declining uranium concentration in the Shihongtan deposit's leaching solutions, a common issue in in-situ leaching (ISL) operations. By analyzing ore mineralogy and conducting controlled batch tests, researchers identified key factors like mineral encapsulation and high carbonate content as causes for poor leaching efficiency. They propose optimized conditions (pH < 6.6, 800 mg/L HCO3⁻) to improve uranium recovery in this and similar deposits.

What Problem Does This Paper Address?

In-situ leaching (ISL) is a widely adopted, cost-effective, and environmentally friendlier method for extracting uranium, particularly from sandstone-type deposits. The process relies on injecting a leaching solution (often CO₂ and O₂) into the ore body to oxidize uranium and complex it into a soluble form that can be pumped to the surface. However, a persistent challenge in ISL, especially in certain regions like the western section of the Shihongtan deposit in Xinjiang, China, is the observed decrease in uranium concentration in the pregnant leach solution over time. This decline directly impacts production efficiency and economic viability. This paper aims to pinpoint the underlying causes for this reduced leaching efficiency and identify optimal operational parameters to overcome this problem.

Methods

The researchers employed a multi-pronged approach:

  • Mineralogical Analysis: Optical microscopy and Scanning Electron Microscopy (SEM) were used to characterize the ore's mineral composition and the form and distribution of uranium minerals. X-ray fluorescence spectrometry was utilized to determine uranium content. This helped understand what was being leached and how it was embedded.
  • Batch Leaching Tests: A series of 16 controlled laboratory experiments were conducted using high-pressure reactors (autoclaves). These tests systematically varied:
  • CO₂:O₂ ratios: Ratios of 1:1, 1:3, 1:7, and 1:10 were tested to understand the impact of oxidant balance.
  • Bicarbonate (HCO₃⁻) concentration: Concentrations ranging from 650 to 1100 mg/L were used, as HCO₃⁻ is crucial for forming soluble uranyl complexes.
  • pH: The pH was controlled within specific ranges (6.2-7.0) to assess its influence on leaching and potential precipitation.
  • Geochemical Modeling: PHREEQCI software was used to calculate the saturation index (SI) of calcite (CaCO₃) and gypsum (CaSO₄) under various conditions. This helped predict and understand potential mineral precipitation that could hinder leaching.

Datasets

The study utilized ore samples collected from the west section of the south ore belt of the Shihongtan uranium deposit in Xinjiang, China. Groundwater samples from the aquifer in the same area were also analyzed for their chemical composition. The paper presents data from 16 batch leaching tests, with results detailed in Appendix A (Tables 1 and 2 for U concentration and leaching rate, respectively, and Tables 3 and 4 for SI of calcite and gypsum). No new benchmark datasets were introduced.

Key Insights and Ideas

  • Uranium Mineralogy is Key: The primary uranium minerals are pitchblende and titanium-bearing uranium minerals. A significant portion of uranium is encapsulated within quartz and other minerals, making it difficult to access and leach. This "hidden" uranium is a major contributor to low recovery.
  • The Double-Edged Sword of Carbonates: While bicarbonate is essential for forming soluble uranium complexes, high concentrations of calcium carbonate and clay minerals in the ore, along with high TDS in groundwater, can reduce porosity and hinder fluid flow. This creates a delicate balance: enough bicarbonate is needed, but too much can lead to problematic precipitation.
  • pH Matters for Precipitation: The study highlights that when the pH exceeds 6.4 and HCO₃⁻ concentration is above 800 mg/L, calcite (CaCO₃) precipitation becomes likely. This precipitation can coat mineral surfaces, further reducing uranium accessibility and leaching efficiency.
  • Oxidant Ratio Fine-Tuning: While CO₂ and O₂ are standard, the specific ratio can influence the process. The paper explores various ratios, suggesting that an optimal balance is needed for effective oxidation and leaching.

Key Results

  • Optimal Leaching Conditions Identified: The study found that a pH lower than 6.6 and a bicarbonate concentration of 800 mg/L yielded the best uranium leaching efficiency.
  • Uranium Concentration Trends: Under the same HCO₃⁻ concentration, uranium concentration generally increased with increasing pH. However, beyond 800 mg/L HCO₃⁻, further increases did not improve, and sometimes even decreased, uranium concentration.
  • Leaching Rate Performance: The uranium leaching rate was found to be between 69% and 79%. It decreased with increasing pH under the same HCO₃⁻ concentration. The highest leaching rate was achieved at 800 mg/L HCO₃⁻.
  • Calcite Precipitation Threshold: Calcite precipitation was predicted to start when pH > 6.4 and HCO₃⁻ concentration > 800 mg/L, indicating a critical window for operational control.

Limitations and Future Work

  • Mineral Encapsulation: The paper acknowledges that uranium minerals mixed with quartz are difficult to activate and recover, suggesting that further research into methods for activating these "locked" uranium resources could be beneficial.
  • Reducing Conditions: The presence of reducing coal or carbon in the ore bed requires sufficient oxidants to activate uranium resources. The study implies that optimizing oxidant addition might be necessary.
  • Flow Field Impact: The paper notes that clay particles can block pore throats, slowing down the flow field. Future work could explore strategies to mitigate this blockage.
  • Generalizability: While the findings are specific to the Shihongtan deposit, the authors suggest that these results can serve as a reference for other similar uranium deposits, implying the need for validation in different geological contexts.

Summary updated

Abstract

CO2 + O2 is a relatively mature, neutral, in situ leaching process that has been widely used. However, the decrease in uranium concentration in the leaching solution during production has become a serious problem in the western section of the south ore belt of the Shihongtan deposit in Xinjiang, China. In order to solve this problem, mineralogy and batch tests were carried out to explore the reason for the low uranium resource leaching efficiency and determine better leaching process parameters. A total of 16 tests were carried out under different conditions of CO2/O2 ratios and HCO3− concentrations. The results show that: (1) The uranium minerals in the ore were mainly pitchblende and titanium-bearing uranium mineral. Part of the uranium resources were mixed in quartz, which were difficult to activate and recover. The high content of calcium carbonate and clay minerals in ore and the high TDS (total dissolved solid) content in groundwater would cause a reduction in porosity. (2) According to the uranium concentration and uranium leaching rate, a better leaching efficiency was obtained when the pH was lower than 6.6, and the HCO3− concentration was 800 mg/L. This result could serve as a reference for production in other similar mines.
BibTeX
@inproceedings{yuan2023study,
  author = {Xin Yuan and Jinhui Liu and Lingling Xu and Yipeng Zhou and Kai Zhao and Mintao Hu},
  title = {{Study on the Leaching Conditions of the Shihongtan Uranium Deposit}},
  booktitle = {Metals},
  year = {2023},
  doi = {10.3390/met13071284},
}
Figure