Structural characterization of radiofrequency magnetron sputter deposited SiO2thin films
Lists
Only you see this
Abstract
The SiO2 thin-film structure deposited by radiofrequency (rf) magnetron sputtering was found to depend on whether the native oxide on the Si(111) was removed or not. X- ray reflectivity (XRR) data show that, when deposited on a clean Si(111) surface, the SiO2 thin film consistently has a two-layer (an overlayer and an interface layer) structure. The interfacial structure depends on the deposition temperature. The film deposited at room temperature has a lower-density interface layer. With increase of the substrate temperature, the density and the thickness of the interface layer also increase. In contrast, when deposited on Si(111) with a native oxide layer, the deposited films have varying structures. At lower temperatures, the XRR data can be fitted with a one-layer model. At higher temperatures, the films consist of two or three layers, including one lower-density top layer, a normal SiO2 layer and a higher-density interface layer. The layer thickness, surface and interface roughness of the two-group samples were also compared and discussed.
BibTeX
@article{li1999structural,
author = {Boquan Li and Toshiyuki Fujimoto and Isao Kojima},
title = {{Structural characterization of radiofrequency magnetron sputter deposited SiO<sub>2</sub>thin films}},
journal = {Journal of Physics D Applied Physics},
year = {1999},
doi = {10.1088/0022-3727/32/12/302},
}Loading related content...