Stress Analysis of Electrochemical and Force-Coupling Model for Ternary Lithium-Ion Batteries

Wei Shi, Ruofan Xu, Changjiang Han, Bingxiang Sun, Jin Chai, Jiachang Liu, Xuewen Jiao, Jiale Xiong, Yinghao LiBatteries 2024 · DOI

TL;DR

This paper presents a novel electrochemical-force coupling model to analyze the internal stress and strain distributions within lithium-ion batteries, crucial for understanding degradation and failure mechanisms. The model reveals that diffusion stress, driven by lithium concentration gradients, is a primary cause of particle rupture, particularly at the negative electrode surface during discharge.

What Problem Does This Paper Address?

Modern electric vehicles rely heavily on lithium-ion batteries, which are often subjected to external mechanical pressure from module assembly. This external pressure, combined with internal stresses generated during battery operation (charging and discharging), can lead to battery degradation and failure. Specifically, the expansion and contraction of electrode materials due to lithium ion intercalation/deintercalation create "diffusion stress." Accurately predicting and understanding this internal stress distribution is challenging because batteries are typically sealed and cannot be easily disassembled for direct measurement. Existing research has focused on external pressure effects or simplified models, leaving a gap in understanding the coupled electrochemical and mechanical behavior at the particle and battery levels. This paper aims to bridge this gap by developing and validating a comprehensive model to predict these internal stresses.

Methods

The authors developed a coupled electrochemical-mechanical model. The electrochemical aspect utilizes a pseudo-two-dimensional (P2D) model, a standard approach for simulating lithium-ion battery behavior. This model captures the conservation of charge and mass, solid-phase diffusion, liquid-phase diffusion, and electrochemical reactions.

The novel contribution lies in coupling this electrochemical model with a mechanical model based on linear elasticity. The key idea is to use the calculated lithium-ion concentration distribution from the electrochemical model to drive the mechanical model. Specifically, the volume changes of electrode active materials due to lithium concentration variations are translated into diffusion stress. This is achieved by:

  • Particle-level stress analysis: Using the diffusion stress-strain relationship derived from linear elasticity and considering the non-uniform lithium concentration within spherical active particles. This allows for the calculation of radial and tangential stresses.
  • Von Mises stress: Employing the Von Mises equivalent stress criterion to predict material failure.
  • Coupling mechanism: The lithium-ion mole flux at the solid-liquid interface, calculated electrochemically, is used to determine the diffusion stress and its impact on particle volume.
  • 3D Simulation: A three-dimensional model is then constructed in COMSOL Multiphysics to analyze the stress and strain distribution across the entire battery, considering external pressure constraints.

Datasets

The study uses a commercial ternary polymer lithium-ion soft-pack cell for its experimental validation. The specific parameters for this cell (voltage, cut-off voltages, etc.) are provided. The model parameters (electrochemical, geometric, and mechanical) are compiled in Table 1, drawing from existing literature and experimental data. No new datasets were introduced; rather, existing data and a specific battery type were used for model development and validation.

Key Insights and Ideas

  • Diffusion stress is the primary driver of internal stress: The paper strongly emphasizes that the internal stress within the battery is predominantly driven by the diffusion of lithium ions and the resulting concentration gradients within active particles, rather than solely external pressure.
  • Negative electrode is most vulnerable: Rupture is most likely to occur at the surface of the negative-electrode active particle, particularly at the end of discharge or the beginning of charging, due to the significant diffusion stress generated by lithium concentration differences.
  • Stress and strain hierarchy: The order of stress and strain within the battery components is consistently found to be: negative active material > negative collector fluid > positive active material > positive fluid. This highlights the critical role of the negative electrode material.
  • External conditions matter significantly: The study demonstrates that discharging rate and ambient temperature have a substantial impact on the Von Mises stress. Higher discharge rates and lower temperatures (below 10°C) lead to significantly increased stress, potentially exceeding the tensile yield strength of graphite anode materials and causing failure.
  • 3D model reveals spatial stress distribution: The 3D simulation shows that stress and strain are concentrated in the peripheral areas of the battery, likely due to structural constraints, while the central region experiences relatively lower stress.

Key Results

  • Model validation: The electrochemical model's voltage predictions showed good agreement with experimental data, with a maximum error of 3.1%. The coupled model's surface pressure prediction had an average error of 19.8% compared to experimental measurements, validating the model's ability to capture mechanical behavior.
  • Stress concentration: The simulation results indicate that the maximum stress occurs in the edge region of the battery, reaching up to 10 MPa at a 1C discharge rate.
  • Impact of discharge rate: Increasing the discharge rate from 0.2C to 1C caused a sharp increase in Von Mises stress, approximately six times the original value. At 2C, stresses exceeded 30 MPa.
  • Impact of temperature: At temperatures below 10°C, diffusion stress was significantly larger than at higher temperatures (20-40°C), exceeding 40 MPa at the end of discharge.

Limitations and Future Work

  • Simplified geometry: The initial analysis focuses on a 1D model and spherical particles, which simplifies the complex geometry of real battery electrodes. While a 3D model is presented, it still relies on idealized representations.
  • Material property assumptions: The model assumes linear elastic behavior for the electrode materials. Real battery materials can exhibit more complex viscoelastic or plastic behaviors, especially under prolonged stress.
  • Experimental limitations: Direct measurement of internal stress and strain in operating batteries remains a significant challenge. The experimental validation relied on indirect measurements like surface pressure.
  • Future work suggested: The authors suggest that the established model can be further developed and parameterized for use in battery management systems. They also imply that understanding these stress distributions can guide the design of more robust battery modules and materials to enhance safety and lifespan. Further investigation into the long-term effects of these stresses on battery performance and degradation mechanisms is also warranted.

Summary updated

Abstract

The mechanical pressure that arises from the external structure of the automotive lithium battery module and its fixed devices can give rise to the concentration and damage of the internal stress inside the battery and increase the risks of battery degradation and failure. Commercial batteries cannot be disassembled, and the diffusion stress distribution at different times during discharge is notoriously difficult to determine. This paper, therefore, establishes the electrochemical force-coupling model based on the electrochemical and diffusion mechanics principles of batteries and studies the internal stress distribution of the battery under the diffusion stress of the electrode-material level and external pressure. Mainly driven by the electrochemical potential of the electrode particle diffusion stress stemming from the lithium-concentration difference inside and outside the particles, rupture is more likely to occur at the surface of the negative-electrode active particle at the end of discharge or the beginning of charging, as shown in simulation analysis. The variation in the volume of electrode material also leads to different stress and strain inside different areas, with the order of strain and stress being negative active material > negative collector fluid > positive active material > positive fluid. Therefore, huge stress and deformation will first cause the negative active particles to deviate from the fluid gradually and squeeze the diaphragm, resulting in mechanical failure accordingly.
BibTeX
@inproceedings{shi2024stress,
  author = {Wei Shi and Ruofan Xu and Changjiang Han and Bingxiang Sun and Jin Chai and Jiachang Liu and Xuewen Jiao and Jiale Xiong and Yinghao Li},
  title = {{Stress Analysis of Electrochemical and Force-Coupling Model for Ternary Lithium-Ion Batteries}},
  booktitle = {Batteries},
  year = {2024},
  doi = {10.3390/batteries10070231},
}
Figure