Spherulite morphology studies of N‐alkyl chitosan films cast from formic acid solutions
Abstract
Abstract The films of N ‐ethyl chitosan were prepared via the solution‐casting technique with formic acid as a solvent. The solutions with different concentrations (35 and 40 wt %) were prepared previously from dilute solution (1 wt %) via evaporating process. The crystalline morphology of these films was investigated by means of polarized optical microscopy and scanning electron microscopy. Normal spherulites with a low growth rate formed in the casting films. The different morphologies of spherulite appeared in the films cast from the solutions with different concentrations. After further crystallizing for a few days, the spherulites were decorated by thousands of needlelike extended‐chain crystals, which had a typical size of ∼50 μm (length) × 2∼5 μm (width) × 1∼2 μm (height) in the central part of the spherulite, but a typical size of ∼5 μm (lenght)× 1∼2 μm (width) × 1∼2 μm (height) in the fringe part of the spherulite. The real concentration for crystallization was determined to be 65–82 wt%. Thus, the crystallization actually appeared in supersaturated solution. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 2033–2038, 2003
BibTeX
@article{dong2003spherulite,
author = {Yanming Dong and Kensuke Sakurai and Yusong Wu and Yukie Kondo},
title = {{Spherulite morphology studies of <i>N</i>‐alkyl chitosan films cast from formic acid solutions}},
journal = {Journal of Polymer Science Part B Polymer Physics},
year = {2003},
doi = {10.1002/polb.10539},
}Ask Althea to put this paper to the test.