Solid reaction between Al and B4C
Abstract
In the present work, solid reaction products formed by a mixture of aluminium and boron carbide (B4C) powder heat treated under low pressure were studied. No significant reaction between B4C and Al could be detected for reaction temperatures of 600°C or less. However, at 640°C, and over a short treatment time (1 h), a solid reaction took place between boron carbide and aluminium with the formation of A13BC and AlB2. Meanwhile, over a longer treatment time (36 h), the detectable product phase between boron carbide and aluminium was AlB12.
BibTeX
@inproceedings{wu2014solid,
author = {Siyuan Wu and Gang Xiao and Xue Li and Ming Zhai and Weiling Zhu and L. Xue and M. Zhai and W. Zhu},
title = {{Solid reaction between Al and B<sub>4</sub>C}},
booktitle = {Canadian},
year = {2014},
doi = {10.1179/1879139514y.0000000178},