Abstract
The groove bottom stress concentration situations of four kinds of groove bars are analyzed by FEM(finite element method).It is determined that the V-shaped groove is the best groove type for fatigue crack initiation during bar stress cut-off.The influences of parameters of V-shaped groove on the bar stress concentration are analyzed,such as groove depth,groove opening angle and groove root radius.The best for the bar stress cut-off are the value of relative groove depth t/d around 0.1,the groove opening angle between 60° and 90° and the groove root radius around 0.2 mm.