SiC ceramics doped with five ratios of ZrO2 short fibers (0, 5, 10, 15, 20 vol.%) were fabricated via hot pressing at 1800°C for 60 min under a pressure of 50 MPa. The bending strength and fracture toughness were improved by ZrO2 short fibers additives except SiC/20 vol.% ZrO2. Moreover, the SiC/15 vol.% ZrO2 possessed the bending strength of 553 ± 30 MPa and fracture toughness of 7.4 ± 0.4 MPa·m−1/2, respectively. However, the relative density decreased. The relative density of pure SiC sample was 94.18%, and the hardness decreased from 13.01 to 12.13 GPa with the increase of the ZrO2 short fiber additive. The ZrC peak was detected in X-ray diffraction patterns, which is the result of the reaction between ZrO2 fibers and SiC.
BibTeX
@article{zhang2016processing,
author = {Liu Zhang and Qinggang Li and Zhi Wang and Shifeng Huang and Xin Cheng},
title = {{Processing and mechanical properties of silicon carbide-based ceramics doped with short zirconia fibers}},
journal = {Journal of the Ceramic Society of Japan},
year = {2016},
doi = {10.2109/jcersj2.15207},
}Loading related content...