Preparation and mechanical behavior of Yb 2 Si 2 O 7 interphase in SiC f /SiC minicomposites
Abstract
Abstract In this work, the Yb 2 Si 2 O 7 interphase was prepared on SiC fibers using the sol–gel method. The influence of sol concentration on the morphology of the interphase was discussed. After heat treatment in argon at 1200°C for 1 h, the Yb 2 Si 2 O 7 was grown in situ on the fiber surface, forming an interphase layer. Then, SiC f /Yb 2 Si 2 O 7 /SiC minicomposites were prepared by chemical vapor infiltration (CVI). The Yb 2 Si 2 O 7 interphase exhibited no changes throughout the high‐temperature preparation process and maintained stability and compatibility with the fiber and matrix. The tensile strength of SiC f /Yb 2 Si 2 O 7 /SiC minicomposites with Yb 2 Si 2 O 7 interphase was significantly higher than SiC f /SiC minicomposites without interphase. The crack deflection, interfacial debonding, and fiber pullout were observed in the tensile fracture of the SiC f /Yb 2 Si 2 O 7 /SiC minicomposites.
BibTeX
@article{mu2024preparation,
author = {Shuang Mu and Qin Ma and Yu Zhang and Xu Shen and Chunjing Liao and Xiangyu Zhang and Yusheng Ding and Shaoming Dong and Jinshan Yang},
title = {{Preparation and mechanical behavior of Yb <sub>2</sub> Si <sub>2</sub> O <sub>7</sub> interphase in SiC <sub>f</sub> /SiC minicomposites}},
journal = {Journal of the American Ceramic Society},
year = {2024},
doi = {10.1111/jace.20153},
}Ask Althea to put this paper to the test.