Durability is an issue for selective catalytic reduction (SCR) catalysts due to their susceptibility to sulfur and water poisoning. In this study, Nano-Ce10-PSDCHF/ZrO2 was prepared by the hydrothermal method using sintering dust, and the impact of SO2 or water vapor on its SCR performance was investigated. The denitrification performance of Nano-Ce10-PSDCHF/ZrO2 was better than that of 0.25-Ce10-PSDCHF/ZrO2 prepared by the impregnation method in the entire temperature interval from 80 to 400 °C. The highest denitrification rate of 93.6% was achieved at 280 °C. Nano-Ce10-PSDCHF/ZrO2 had a smaller particle size and uniform dispersion but also formed a high concentration of Ce3+ and adsorbed oxygen Oα on the surface. Additionally, it showed better resistance to water and sulfur than 0.25-Ce10-PSDCHF/ZrO2. Even when exposed to 8% H2O and 400 ppm SO2, the denitrification rate of Nano-Ce10-PSDCHF/ZrO2 remained at 82.1% after 4 h. SO2 is more toxic to SCR catalysts than H2O. The effect of water on catalyst activity is partially reversible. Deactivation of SCR by SO2 is primarily caused by the formation of ammonium sulfate species, with some contribution from competitive adsorption between SO2 and NOx. In conclusion, the Nano-Ce10-PSDCHF/ZrO2 catalyst exhibited the best SCR performance, with water and sulfur resistance, and effectively utilized sintering dust, which has potential application value.
BibTeX
@inproceedings{li2023performance,
author = {Zetong Li and Shuaipeng Li and Yue Zhou and Yaru Wang and Dazhan Jiang and Zhenting Chen and Keying Zhu and Shengwen Chen and Zhiguo Sun},
title = {{Performance of an SCR Catalyst from Sintering Dust by the Hydrothermal Method and Its Water/Sulfur Resistance}},
booktitle = {Energy},
year = {2023},
doi = {10.1021/acs.energyfuels.3c01578},
}Loading related content...