Low‐Temperature Synthesis of CaZrO 3 Powder from Molten Salts

Zushu Li, William Lee, Shaowei ZhangJournal of the American Ceramic Society 2007

Abstract

Calcium zirconate (CaZrO 3 ) powder was synthesized using calcium chloride (CaCl 2 ), sodium carbonate (Na 2 CO 3 ), and zirconia (ZrO 2 ) powders. On heating, CaCl 2 reacted with Na 2 CO 3 to form NaCl and CaCO 3 . NaCl–Na 2 CO 3 molten salts provided a liquid reaction medium for the formation of CaZrO 3 from in situ ‐formed CaCO 3 (or CaO) and ZrO 2 . CaZrO 3 started to form at about 700°C, increasing in amount with increasing temperature and reaction time, with a concomitant decrease in CaCO 3 (or CaO) and ZrO 2 contents. After washing with hot‐distilled water, the samples heated for 5 h at 1050°C were single‐phase CaZrO 3 with 0.5–1.0 μm grain size.
BibTeX
@article{li2007lowtemperature,
  author = {Zushu Li and William Lee and Shaowei Zhang},
  title = {{Low‐Temperature Synthesis of CaZrO <sub>3</sub> Powder from Molten Salts}},
  journal = {Journal of the American Ceramic Society},
  year = {2007},
  doi = {10.1111/j.1551-2916.2006.01383.x},
}

Loading related content...