Low-Temperature Plasma-Enhanced Atomic Layer Deposition of ZnMgO for Efficient CZTS Solar Cells
Lists
Only you see this
Abstract
Cu2ZnSnS4 (CZTS) solar cells are an emerging photovoltaic technology owing to their earth abundance, all-dry processability, and environmental friendliness. Further power conversion efficiency enhancement of the Cd-free CZTS device necessitates the substitution of traditionally used intrinsic ZnO by an alternative wide-band-gap window layer. Here, we demonstrate deposition of a ZnMgO window layer of controlled thickness, composition, and electro-optical properties by atomic layer deposition (ALD). The amorphous ZnMgO deposited at low temperature down to 100 °C using plasma-enhanced ALD showed smoothness superior to that of high-temperature plasma-enhanced ALD and doping density comparable to that of high-temperature thermal ALD but with a much lower electron affinity. The overall charge carrier recombination at the CZTS/ZnSnO/ZnMgO region was reduced due to the optimized ZnMgO conduction band minimum, thus reducing the VOC value and fill factor loss for a CZTS solar cell. In addition, the thinner- and larger-band-gap ZnMgO was believed to reduce the parasitic absorption, improving the JSC value and boosting the efficiency to 10%.
BibTeX
@inproceedings{cui2023low,
author = {Xin Cui and Kaiwen Sun and Jialiang Huang and Heng Sun and Ao Wang and Xiaojie Yuan and Martin A. Green and Bram Hoex and Xiaojing Hao},
title = {{Low-Temperature Plasma-Enhanced Atomic Layer Deposition of ZnMgO for Efficient CZTS Solar Cells}},
booktitle = {ACS},
year = {2023},
doi = {10.1021/acsmaterialslett.2c01203},
}Loading related content...