TL;DR
Researchers have developed a novel method for creating ultrathin, high-resolution resist films for microlithography using the Langmuir-Blodgett (LB) technique with polymethylmethacrylate (PMMA). This approach successfully achieved 0.15 µm line-and-space patterns, demonstrating its potential for fabricating advanced microelectronic devices and masks.
What Problem Does This Paper Address?
The relentless drive towards miniaturization in microelectronics, exemplified by the development of high electron mobility transistors and surface acoustic wave devices, demands increasingly sophisticated lithography techniques. While electron beam lithography offers high resolution and maskless patterning, its effectiveness is limited by the proximity effect, which becomes more pronounced with thicker resist films. Conventional spin-casting methods struggle to produce high-quality ultrathin films (below 300 nm) with low pinhole density and sufficient etch resistance. This paper addresses the need for a reliable method to create ultrathin, high-resolution resist films that overcome these limitations, paving the way for sub-micron lithography.
Methods
The core innovation lies in the use of Langmuir-Blodgett (LB) films of polymethylmethacrylate (PMMA) as electron beam resists. PMMA, a common polymer, was dissolved in trichloromethane and spread onto a water surface. The hydrophilic groups were oriented towards the water, while the backbone lay parallel to the surface. This monolayer was then transferred onto silicon wafers coated with a thin aluminum film using the Wilhelmy plate method at a controlled surface pressure. The LB technique allowed for precise control over film thickness, with each layer adding approximately 0.85 nm.
For exposure, a modified scanning electron microscope (SEM) was employed. This custom setup, based on a Hitachi S-450 SEM, was computer-controlled for high-resolution electron beam lithography. The system allowed for precise control of beam diameter (as low as 7 nm), beam current, and scanning time to manage the exposure dose. After exposure, the PMMA resist was developed using a mixture of methyl isobutyl ketone (MIBK) and isopropyl alcohol (IPA). Finally, the underlying aluminum film was etched using a phosphoric acid solution, and the remaining PMMA was stripped with acetone. Atomic force microscopy (AFM) was used to assess the quality of the patterned films, particularly for pinhole detection.
Datasets
Not discussed in the paper. The paper focuses on experimental results using prepared resist films and substrates.
Key Insights and Ideas
- LB films as a viable ultrathin resist: The LB technique offers superior control over film thickness and quality compared to spin-casting for creating ultrathin resists, crucial for mitigating proximity effects in electron beam lithography.
- PMMA's suitability for LB lithography: Despite not being inherently amphiphilic like some other LB resist materials, PMMA demonstrated good robustness and etch resistance when prepared using the LB method with specific processing steps.
- Importance of processing parameters: The paper highlights the critical role of baking steps during LB film deposition in enhancing adhesion between layers and the substrate, which in turn improves etch resistance.
- SEM as a high-resolution lithography tool: The modified SEM proved capable of achieving sub-micron resolution, demonstrating the potential of repurposing SEMs for advanced lithography applications.
- Good etch resistance: The ultrathin PMMA LB films exhibited sufficient etch resistance to transfer patterns to the underlying aluminum layer, a key requirement for mask fabrication.
Key Results
- Resolution: The study successfully achieved 0.15 µm lines and spaces, demonstrating the capability of the LB PMMA resist and the modified SEM system for sub-micron lithography.
- Pinhole density: AFM analysis revealed very few apparent large pinholes, with the largest observed being less than 15 nm in diameter, indicating high-quality film preparation.
- Etch resistance: The resist demonstrated good etch resistance, allowing for the transfer of patterns to a 100 nm aluminum film.
- Dose-resolution relationship: The paper showed that pattern resolution could be improved by adjusting the exposure dose, with resolutions changing from 0.45 µm to 0.15 µm as the dose was varied.
Limitations and Future Work
The authors acknowledge that the achieved exposure conditions might not have been entirely optimal due to limitations of the experimental setup. They suggest that further optimization of exposure parameters could potentially lead to even higher resolutions. Future work could explore the use of other amphiphilic molecules in LB films for electron beam lithography, as well as investigate the application of this technique for fabricating specialized devices and masks. The study also implies that further research into the exact mechanisms of adhesion enhancement through baking and the etch resistance of LB PMMA films would be beneficial.
Summary updated