TL;DR
This paper investigates the formation and healing of cracks in thick GaN films grown using a novel combined MOCVD-HVPE technique. They found that cracks originate during the growth process due to accumulated tensile stress and are subsequently healed by lateral growth, rather than extending to the film surface or substrate.
What Problem Does This Paper Address?
Gallium Nitride (GaN) is a crucial material for optoelectronic and high-power electronic devices, often grown as epitaxial films on foreign substrates like sapphire. The significant differences in thermal expansion coefficients (TEC) and lattice constants between GaN and these substrates lead to substantial residual stress in thick GaN films. This stress can cause cracking, which degrades device performance and yield. While hydride vapor-phase epitaxy (HVPE) is a cost-effective method for growing thick GaN, cracks are a common issue. This paper aims to understand the origin, distribution, and healing mechanism of these cracks in GaN films grown by a combined MOCVD-HVPE approach, which offers advantages like in-situ process control and reduced contamination.
Methods
The researchers employed a multi-pronged approach to characterize the GaN films:
- Combined MOCVD-HVPE Growth: A novel system integrated both techniques in a single chamber, allowing for the deposition of a GaN buffer layer by MOCVD followed by a thick GaN layer by HVPE.
- High-Resolution X-ray Diffraction (HR-XRD): Used to determine the overall crystal quality (rocking curves) and lattice constants, providing insights into strain.
- Scanning Electron Microscopy (SEM): Employed to observe the surface morphology and the cross-section of the films, revealing the presence and extent of cracks. Etching was used to expose subsurface cracks.
- Micro-Raman Spectroscopy: A powerful tool for probing stress distribution within the film. By scanning along the depth of the film, they mapped the stress profile. The frequency of the E2 (high) phonon mode is particularly sensitive to in-plane strain.
- Cathodoluminescence (CL): Used to reveal the effects of grain boundaries and dislocations on crack formation and propagation.
- Cleaving and Etching: Cross-sections were prepared by cleaving and then lightly etched to compare the crystal quality of healed crack regions with uncracked areas.
Datasets
Not discussed in the paper. The study focuses on the characterization of GaN films grown in their laboratory.
Key Insights and Ideas
- Cracks Originate During Growth, Not Cooling: Contrary to some previous hypotheses, the evidence strongly suggests that the cracks form during the growth process itself, when accumulated tensile stress exceeds a critical threshold, rather than solely due to thermal stress during cooling.
- Subsurface Cracks are the Norm: SEM analysis after etching revealed that cracks are primarily located within the film, not extending to the surface or the substrate interface.
- Healing by Lateral Growth: The observation that the crystal quality of healed crack regions is comparable to uncracked areas, coupled with the morphology of the crack edges, points to a significant lateral growth rate that effectively "heals" the cracks during subsequent growth.
- Complex Stress Profile: Micro-Raman depth profiling revealed a non-monotonic stress distribution, with compressive stress at the interface, a decrease, a sustained high value, another decrease, and a final increase near the surface. This complex profile likely contributes to the crack formation and healing dynamics.
- Limited Interaction with Defects: CL mapping indicated that cracks do not appear to interact significantly with grain boundaries or dislocations, suggesting that the primary driver for cracking is the overall film stress.
Key Results
- Cracks were observed in a 22-µm thick GaN film grown by the combined MOCVD-HVPE method.
- SEM images showed cracks that were perpendicular to the film/substrate interface, pinched off at locations, and did not extend to the surface or substrate.
- Micro-Raman spectroscopy revealed a complex stress distribution along the film depth.
- Etching of cleaved cross-sections showed that healed crack regions had crystal quality similar to uncracked regions.
Limitations and Future Work
- Limited Substrate Scope: The study focused on GaN grown on sapphire. Further investigation on other substrates would be valuable.
- Specific Growth Conditions: The findings are specific to the combined MOCVD-HVPE parameters used. Optimizing these parameters for crack-free growth remains an area for exploration.
- Quantitative Healing Mechanism: While lateral growth is proposed as the healing mechanism, a more quantitative analysis of the healing rate and its dependence on growth parameters could be beneficial.
- Impact on Device Performance: While cracks are detrimental, the paper doesn't quantify the specific impact of these healed cracks on device performance. Future work could focus on correlating crack characteristics with device electrical and optical properties.
Summary updated