Improving the Efficiency of Semitransparent Perovskite Solar Cell Using Down-Conversion Coating

Damian Głowienka, Chieh-Ming Tsai, A. Sbai, Dian Luo, Pei‐Huan Lee, Shih‐Han Huang, Chia‐Feng Li, Haowen Wang, Guey‐Sheng Liou, Julien Guthmuller, Wei‐Fang SuACS 2024 · DOI

TL;DR

Researchers have developed novel down-conversion coatings for semitransparent perovskite solar cells (PSCs) that convert high-energy UV light into usable visible light. By optimizing the thickness and placement of these coatings, they achieved a significant efficiency boost of approximately 0.4%, demonstrating a promising strategy to push PSCs closer to their theoretical performance limits.

What Problem Does This Paper Address?

Perovskite solar cells (PSCs) have seen remarkable efficiency gains, but they still fall short of their theoretical maximum efficiency (around 33.7% for a 1.33 eV bandgap). A major hurdle is optical loss, where a significant portion of incident solar energy (over 40%) is not converted into electricity. This loss occurs due to parasitic absorption within the cell layers or because photon energies are too low to be absorbed. Specifically, high-energy UV light, which constitutes about 5% of solar energy and can also degrade the perovskite material, is often poorly utilized or even harmful. This paper tackles the challenge of reducing these optical losses, particularly UV absorption, by employing down-conversion techniques to convert this wasted energy into a more usable form.

Methods

The study combines experimental fabrication and characterization with advanced optical modeling.

  • Down-Conversion Material Development: Two organic molecules exhibiting aggregation-induced emission (AIE) – N,N-diphenyl-4-(1,2,2-triphenylethenyl)-benzenamine (TPETPA) and 4-(N,N-diphenylamino)benzaldehyde (DPABA) – were chosen. These were mixed with a polymeric binder (TFEVE) to create thin films. AIE is crucial as it enhances fluorescence when molecules aggregate, a behavior beneficial for photovoltaic applications.
  • Device Fabrication: Semitransparent PSCs were fabricated using a standard layered architecture (glass/ITO/NiOx/P3HT-COOH/perovskite/PCBM/SnO2/ICO). The down-conversion layers were then applied to either the front or rear side of these devices.
  • Optical Modeling: A generalized transfer-matrix (GTM) optical model was employed to meticulously analyze optical losses (reflection, transmission, parasitic absorption) within the PSC stack under front and rear illumination. This model was refined by incorporating experimental data from ellipsometry and UV-vis spectroscopy to determine the complex refractive indices of each layer.
  • Characterization:
    • UV-vis and Photoluminescence (PL) Spectroscopy: Used to characterize the absorption and emission properties of the down-conversion films.
  • External Quantum Efficiency (EQE): Measured to assess the spectral response of the PSCs with and without the down-conversion layers.
  • Current-Voltage (J-V) Measurements: Performed under AM1.5G solar simulation to determine key photovoltaic parameters like PCE, Jsc, FF, and Voc.
  • Quantum Chemical Calculations (TDDFT): Density Functional Theory was used to understand the electronic transitions governing the absorption and emission of the AIE molecules.

Datasets

Not discussed in the paper. The study focuses on experimental data generated from fabricated devices and materials, alongside optical simulations.

Key Insights and Ideas

  • AIE Molecules as Efficient Down-converters: The chosen AIE molecules (TPETPA and DPABA) effectively absorb UV light and re-emit it in the visible spectrum, demonstrating their potential for enhancing PSC performance.
  • Importance of Aggregation: The AIE phenomenon, where luminescence increases upon aggregation, is key to the effectiveness of these organic dyes within the polymeric binder.
  • Front vs. Rear Illumination Losses Differ: Significant optical losses occur on the front side due to UV absorption by glass and ITO, while rear-side losses are dominated by the top ICO electrode. This necessitates tailored approaches for each side.
  • Thickness Optimization is Crucial: The thickness of the down-conversion layer is a critical parameter. Too thin, and it may not absorb enough UV; too thick, and it can introduce parasitic absorption losses in the visible spectrum.
  • Down-conversion Layer Placement Matters: Different materials (ZE10 for front, ZD20 for rear) were found to be optimal for their respective positions, leveraging their specific absorption/emission characteristics.
  • PLQY vs. Realized Quantum Yield: While initial PLQY measurements of the films were high (50-60%), the actual quantum yield realized within the PSC stack was significantly lower (16-30%), highlighting the importance of considering device integration and light management within the cell. A substantial portion of emitted light can be lost at the edges of the coating.

Key Results

  • Efficiency Improvement: Application of optimized ZE10 (front) and ZD20 (rear) down-conversion layers resulted in a notable increase in power conversion efficiency (PCE) of approximately 0.4% for semitransparent PSCs.
  • ZE10 (front): PCE increased from 13.01% to 13.40% (a gain of 0.39%).
  • ZD20 (rear): PCE improved from 9.88% to 10.27% (a gain of 0.39%).
  • Short-Circuit Current Density (Jsc) Enhancement:
    • ZE10 (front): Jsc increased by 0.54 ± 0.04 mA cm⁻².
  • ZD20 (rear): Jsc increased by 0.18 ± 0.03 mA cm⁻².
  • Open-Circuit Voltage (Voc) Improvement:
    • ZE10 (front): Voc increased by approximately 20 mV (from 979 mV to 999 mV).
  • ZD20 (rear): Voc increased by approximately 9 mV (from 942 mV to 951 mV).
  • Optimal Thicknesses: Determined optimal thicknesses were 350 nm for ZE10 (front) and 400 nm for ZD20 (rear).
  • UV Light Mitigation: The ZE10 layer showed a modest EQE increase (~10%) in the UV range, while ZD20 achieved up to an 8% EQE increase in the 300-350 nm range.

Limitations and Future Work

  • Realized Quantum Yield: A significant limitation identified is that only a fraction (approximately one-fourth) of the light emitted by the down-conversion layer is effectively harnessed by the solar cell. The rest is lost at the edges or through other pathways.
  • Parasitic Absorption: While down-conversion helps with UV, thicker layers can introduce parasitic absorption in the visible spectrum, necessitating careful thickness optimization.
  • Future Work: The authors emphasize the need for improving techniques for studying and optimizing down-conversion materials. Further research could focus on better light management strategies to capture more of the down-converted light, potentially leading to even greater efficiency gains. Exploring new AIE materials with tailored spectral properties and improved integration into PSC architectures would also be beneficial.

Summary updated

Abstract

Perovskite solar cells (PSCs) have demonstrated exceptional efficiency, yet surpassing theoretical performance limits requires innovative methodologies. Among these, down-conversion techniques are pivotal in reducing optical losses and enhancing energy conversion efficiency. In this study, optical modeling, including a generalized transfer-matrix optical model, was employed to meticulously assess optical losses in semitransparent PSCs illuminated from the front and rear sides of the device. To reduce these losses, two down-conversion layers, made of <i>N</i>,<i>N</i>-diphenyl-4-(1,2,2-triphenylethenyl)-benzenamine and 4-(<i>N</i>,<i>N</i>-diphenylamino)benzaldehyde mixed with polymeric binder, were developed, showcasing initial photoluminescence quantum yields of 60% and 50% as films, respectively. The materials luminescence relies on the effect of aggregation-induced emission, which enhances the fluorescence of the dyes within the binder, providing their films with a unique behavior beneficial for photovoltaic applications. An optimization of these layers was performed, which aimed to reduce UV optical losses by adjusting the film thickness atop the PSCs. The refined down-conversion layers yielded a notable increase in the power conversion efficiency by approximately 0.4% for both the front and rear sides of the PSCs, demonstrating their significant potential in pushing the boundaries of solar cell performance.
BibTeX
@inproceedings{gowienka2024improving,
  author = {Damian Głowienka and Chieh-Ming Tsai and A. Sbai and Dian Luo and Pei‐Huan Lee and Shih‐Han Huang and Chia‐Feng Li and Haowen Wang and Guey‐Sheng Liou and Julien Guthmuller and Wei‐Fang Su},
  title = {{Improving the Efficiency of Semitransparent Perovskite Solar Cell Using Down-Conversion Coating}},
  booktitle = {ACS},
  year = {2024},
  doi = {10.1021/acsami.4c12551},
}
Figure