Identifying Faulty Electrical Contact Points in Li-Ion Battery Packs

Xulai Yang, Wenjing Yang, Rui XueJournal of The Electrochemical Society 2022 · DOI

TL;DR

This paper investigates how faulty electrical contact points (FECPs)—essentially "bad connections"—cripple the performance and lifespan of lithium-ion battery packs. The researchers demonstrate that these faults produce distinct thermal and voltage signatures depending on whether they occur in series or parallel circuits, providing a roadmap for earlier detection and improved pack safety.

What Problem Does This Paper Address?

While much research focuses on the electrochemical degradation of individual battery cells, the "glue" that holds a pack together—the electrical connections—is often overlooked. In large-scale battery packs for electric vehicles (EVs), hundreds of cells are joined via welding or mechanical fasteners.

A single "loose" or faulty connection (FECP) introduces parasitic resistance. This doesn't just waste energy; it generates localized heat (Joule heating) and causes current imbalances. These imbalances force some cells to work harder than others, leading to premature pack failure, sudden drops in state-of-charge (SOC), and potential thermal runaway. The challenge is that these faults are often "invisible" to standard management systems until it's too late.

Methods

The authors constructed experimental battery packs using 30 Ah LiFePO4/graphite prismatic cells in two configurations: 1p3s (1 parallel, 3 series) and 3p3s (3 parallel, 3 series).

To simulate "faulty" contacts in a controlled way, they used screw-type connectors instead of permanent welds, adjusting the tightness to achieve specific contact resistances (ranging from ~0.4 mΩ to ~2.0 mΩ). They then subjected these packs to rigorous cycling (1.0C rate) while monitoring 32 channels of high-precision voltage and temperature data. This allowed them to compare "healthy" packs (low, uniform resistance) against those with intentional FECPs in either series or parallel positions.

Datasets

The study generated its own experimental data. It did not use external training datasets. The primary data points included:

  • Voltage/Temperature Evolutions: Time-series data during charge/discharge cycles.
  • Cycle Life Data: Capacity retention over 1,500+ cycles.
  • Connector Impedance (CI): Measured via multimeter with ±0.5% accuracy.

Key Insights and Ideas

  • The "Thermal Signature" Difference:
    • In series circuits, a faulty contact heats up instantaneously as soon as current flows.
  • In parallel circuits, the heat spike is delayed. It only appears near the "voltage turning point" (the end of the charge or discharge process). This is because current naturally avoids the high-resistance path until the other parallel cells are nearly full/empty, at which point the current is forced through the faulty contact.
  • Voltage Polarization as a Diagnostic: FECPs significantly increase the "Medium-Voltage Difference" (MVD) between cells. A high MVD during the middle of a cycle is a strong indicator of a connection issue rather than a cell chemistry issue.
  • The "Platform Shift": Packs with FECPs exhibit higher charge voltage platforms and lower discharge voltage platforms. This "widening" of the voltage gap is a hallmark of parasitic resistance.
  • Series vs. Parallel Severity: A faulty contact in a series string is far more damaging than one in a parallel block. It acts as a bottleneck for the entire pack's current, leading to much faster degradation.

Key Results

  • Drastic Life Reduction: A healthy 1p3s pack reached 80% capacity after 1,260 cycles. The same pack with a modest FECP (0.42 mΩ) in the series circuit failed at just 381 cycles.
  • Parallel Impact: A 3p3s pack with a parallel FECP (0.41 mΩ) lasted 1,097 cycles, showing that while parallel faults are less immediately destructive than series faults, they still significantly underperform compared to healthy packs (~1,210 cycles).
  • Temperature Extremes: In some tests, a faulty contact reached 80°C in a short time during 1C discharge, highlighting the severe fire risk posed by poor connections.
  • Detection Window: The researchers identified that the end-of-discharge voltage difference (VDwED) is a highly sensitive feature for identifying packs harboring faulty contacts.

Limitations and Future Work

The authors acknowledge a few constraints:

  • Manual Simulation: Using screws to simulate faults is a good experimental proxy, but real-world faults (like cracked welds or corrosion) might have more complex, non-linear resistance behaviors.
  • Chemistry Specificity: The study focused on LiFePO4 (LFP) cells. While the electrical principles are universal, the specific voltage "turning points" and thermal sensitivities might differ for NCM or NCA chemistries.
  • BMS Integration: While the paper identifies how to see these faults, it does not provide a specific algorithm for a Battery Management System (BMS) to distinguish between a bad cell and a bad connection in real-time.

Future research could focus on developing automated diagnostic software that uses these thermal and voltage signatures to alert EV owners to "loose bolts" before they lead to pack failure.

Summary updated

Abstract

The cell-to-cell electrical contact resistance was investigated to estimate the effect of faulty electrical contact point(FECP) on the performance of battery packs. The temperature of the FECP in series circuit rises instantaneously compared to that of other normal points after the start of the current load, but the temperature of the FECP in parallel circuit rises just after the voltage turning point at the end of the charging/discharging process. The voltage difference between the highest voltage and the lowest voltage of the cells at the end of discharge stage increases apparently while the battery pack contains the FECPs, which is a typical feature during the decay of battery packs. In this study, the capacity retention of LiFePO 4 /C battery at room temperature reaches to 80% after 1260 cycles for a 1p3s pack, 1210 cycles for a 3p3s pack and 1510 cycles for a single cell, in which the average cell-to-cell connector impedance is 0.13 mΩ in the circuit. By contrast, the cyclic charge-discharge stops at 381st cycle for a 1p3s pack with a FECP(0.42 mΩ) in series circuit and at 1097th cycle for a 3p3s pack with a FECP(0.41 mΩ) in parallel circuit.
BibTeX
@article{yang2022identifying,
  author = {Xulai Yang and Wenjing Yang and Rui Xue},
  title = {{Identifying Faulty Electrical Contact Points in Li-Ion Battery Packs}},
  journal = {Journal of The Electrochemical Society},
  year = {2022},
  doi = {10.1149/1945-7111/ac9a02},
}
Figure