High-Quality Alloyed CdSxSe1-x Whiskers as Waveguides with Tunable Stimulated Emission

Anlian Pan, Ruibin Liu, Feifei Wang, Sishen Xie, Bingsuo Zou, Margit Zacharias, Zhong Lin WangThe Journal of Physical Chemistry B 2006 · DOI

TL;DR

Researchers have developed a method to grow high-quality, alloyed CdSxSe1-x semiconductor whiskers that act as efficient optical waveguides. These whiskers exhibit tunable stimulated emission across the visible spectrum (green to red) by simply adjusting their composition, paving the way for new tunable nano/micro-lasers.

What Problem Does This Paper Address?

The development of miniaturized, tunable light sources is a significant challenge in photonics and optoelectronics. While 1D semiconductor nanostructures like nanowires and whiskers have shown promise as components for lasers and waveguides, a key limitation has been the inability to tune their emission wavelength. This is particularly true for binary semiconductors, where the band gap and thus emission color are fixed. This paper addresses this by exploring ternary alloys, specifically CdSxSe1-x, aiming to achieve tunable emission by controlling the sulfur-to-selenium ratio within the whiskers, while also ensuring they function effectively as optical waveguides.

Methods

The researchers synthesized CdSxSe1-x whiskers using a multistep thermal evaporation technique. This involved placing CdS and CdSe powders in a quartz tube furnace and heating them under a controlled flow of helium gas. Silicon substrates coated with a thin gold film were placed downstream to act as nucleation sites for whisker growth. The composition of the whiskers was tuned by adjusting the molar ratio of CdS to CdSe in the source powder.

Characterization techniques included:

  • Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) for morphology and elemental composition.
  • Transmission Electron Microscopy (TEM) and Selected Area Electron Diffraction (SAED) for crystal structure and quality.
  • X-ray Powder Diffraction (XRD) for crystallographic phase and lattice parameter determination.
  • UV-vis reflectance spectroscopy to determine band gap energies.
  • Optical waveguide properties were investigated using a scanning near-field optical microscope (NSOM) with continuous-wave (CW) laser excitation.
  • Stimulated emission measurements were performed using pulsed laser excitation (third harmonic of Nd:YAG laser) at room temperature, with photoluminescence (PL) detected by a spectrometer.

Datasets

Not discussed in the paper. The study focuses on the synthesis and characterization of novel materials.

Key Insights and Ideas

  • Compositional Tuning is Key: The ability to tune the sulfur-to-selenium ratio in CdSxSe1-x whiskers directly translates to a tunable band gap and, consequently, a tunable emission wavelength. This is a significant advantage over binary semiconductor nanostructures.
  • Whiskers as Efficient Waveguides: The synthesized CdSxSe1-x whiskers, with their uniform width and clean surfaces, act as excellent optical waveguides. They can effectively guide light emitted from their near-band edge over sub-millimeter distances.
  • Stimulated Emission Achieved: Under pulsed laser excitation, these whiskers exhibit stimulated emission, a prerequisite for lasing. This was observed across the entire compositional range (0 ≤ x ≤ 1) at room temperature.
  • Low Lasing Thresholds: The whiskers demonstrate remarkably low lasing thresholds, comparable to or better than other 1D nanostructures and significantly lower than platelet lasers or quantum dots in microcavities. This is attributed to their high optical confinement, continuous gain medium along the axis, and their natural Fabry-Pérot cavity formation due to cleaved end facets.
  • Potential for Tunable Nano/Micro-Lasers: The combination of waveguide properties and tunable stimulated emission makes these CdSxSe1-x whiskers highly promising building blocks for compact, adjustable laser sources.

Key Results

  • High-quality, ultralong CdSxSe1-x whiskers with uniform rectangular cross-sections (approx. 600 nm x 5 µm) were synthesized.
  • The band gap of the whiskers could be continuously tuned from ~2.49 eV (CdS) to ~1.77 eV (CdSe) by varying the S/Se ratio.
  • Near-band-edge emission was effectively guided along the whiskers at the sub-millimeter scale under CW laser excitation.
  • Stimulated emission was observed in all CdSxSe1-x compositions (0 ≤ x ≤ 1) at room temperature, with spectral positions tunable from green to red.
  • Lasing thresholds were found to be low, typically in the range of tens of kW/cm², and comparable to binary CdS and CdSe whiskers.

Limitations and Future Work

Limitations: * The paper mentions that the whiskers have sharp cleaved end facets due to the sonication process used to detach them from the substrate. While beneficial for forming Fabry-Pérot cavities, this detachment process might introduce some surface defects. * The paper doesn't explicitly discuss the long-term stability or efficiency of these structures in practical device applications.

Future Work: * The authors suggest that these CdSxSe1-x whiskers have potential applications in adjustable nano/micro-lasers. Further research could focus on integrating these whiskers into functional laser devices. * Exploring different fabrication techniques or post-processing methods to potentially improve surface quality or control end facet reflectivity could be beneficial. * Investigating the performance of these structures under different excitation conditions or in more complex optical setups would be valuable.

Summary updated

Abstract

High-quality ultra-long alloyed CdS(x)Se(1)(-)(x) (0 < or = x < or = 1) whiskers were obtained by a simple thermal evaporation route. The near band-edge emission in these whiskers can be effectively guided at the sub-millimeter scale under continuous-wave laser excitation. As good optical waveguide cavities, the whiskers exhibit stimulated emissions under pulsed light excitation at room temperature for all compositions 0 < or = x < or = 1. The spectral positions of the sharp emission lines of the whiskers were tuned by their compositions, covering the spectral range from green to red.
BibTeX
@article{pan2006high,
  author = {Anlian Pan and Ruibin Liu and Feifei Wang and Sishen Xie and Bingsuo Zou and Margit Zacharias and Zhong Lin Wang},
  title = {{High-Quality Alloyed CdS<i><sub>x</sub></i>Se<sub>1-</sub><i><sub>x</sub></i> Whiskers as Waveguides with Tunable Stimulated Emission}},
  journal = {The Journal of Physical Chemistry B},
  year = {2006},
  doi = {10.1021/jp064664s},
}
Figure