Fracture toughness of sodium aluminosilicate hydrate (NASH) gels: Insights from molecular dynamics simulations

Gideon A. Lyngdoh, Sumeru Nayak, Rajesh Kumar, N. M. Anoop Krishnan, Sumanta DasJournal of Applied Physics 2020 · DOI

Abstract

This paper evaluates the fracture toughness of sodium aluminosilicate hydrate (N-A-S-H) gel formed through alkaline activation of fly ash via molecular dynamics (MD) simulations. The short- and medium-range order of the constructed N-A-S-H structures shows good correlation with the experimental observations, signifying the viability of the N-A-S-H structures. The simulated fracture toughness values of N-A-S-H (0.4–0.45 MPa m0.5) appear to be of the same order as the available experimental values for fly ash-based geopolymer mortars and concretes. These results suggest the efficacy of the MD simulation toward obtaining a realistic fracture toughness of N-A-S-H, which is otherwise very challenging to obtain experimentally, and no direct experimental fracture toughness values are yet available. To further assess the fracture behavior of N-A-S-H, the number of chemical bonds formed/broken during elongation and their relative sensitivity to crack growth are evaluated. Overall, the fracture toughness of N-A-S-H presented in this paper paves the way for a multiscale simulation-based design of tougher geopolymers.
BibTeX
@article{lyngdoh2020fracture,
  author = {Gideon A. Lyngdoh and Sumeru Nayak and Rajesh Kumar and N. M. Anoop Krishnan and Sumanta Das},
  title = {{Fracture toughness of sodium aluminosilicate hydrate (NASH) gels: Insights from molecular dynamics simulations}},
  journal = {Journal of Applied Physics},
  year = {2020},
  doi = {10.1063/1.5144876},
}

Loading related content...

Figure