Fracture Analysis on Welding Zone of Aluminum Alloy Thin-wailed Tube
Abstract
After visual inspection and metallographic test,analysis and discuss the welding zone cracking reasons for 6061 and A7003 aluminum alloy thin-walled tube after TIG(argon shielded arc) welding.From which,although the welding properties are not the same for different aluminum alloy brands,but the main reason for such aluminum alloy thin-walled tube cracking was not the material itself,and the instability for energy input in welding caused concavity and convexity to arose hot cracks.
BibTeX
@inproceedings{yu2007fracture,
author = {Hui Yu},
title = {{Fracture Analysis on Welding Zone of Aluminum Alloy Thin-wailed Tube}},
booktitle = {Heat},
year = {2007},
}Ask Althea to put this paper to the test.