Experimental Research on the Impact Resistance Mechanical Properties and Damage Mechanism of Rubberized Concrete under Freeze–Thaw Cycling

Xiaowen Huang, Tengsheng Yue, Jun Zhang, Jinsong ZhangJournal of Composites Science 2024 · DOI

TL;DR

This study investigates how adding waste tire rubber to concrete affects its performance under freeze-thaw cycles and dynamic impact. The findings show that rubberized concrete, particularly with finer rubber particles (30-mesh), exhibits improved frost and impact resistance, maintaining better integrity and experiencing less degradation after repeated freeze-thaw cycles compared to ordinary concrete.

What Problem Does This Paper Address?

High-altitude regions and areas with extreme temperature fluctuations face significant challenges with concrete infrastructure due to the damaging effects of freeze-thaw cycles. Traditional concrete, while strong, can be brittle and prone to cracking and damage under these conditions, leading to costly repairs and reduced service life. Waste tire rubber presents an opportunity to enhance concrete's properties, but its impact on dynamic mechanical behavior, especially after environmental degradation like freeze-thaw, needs thorough investigation for practical engineering applications. This paper aims to fill this gap by systematically evaluating the freeze-thaw and impact resistance of rubberized concrete with varying rubber particle sizes.

Methods

The researchers employed a combination of experimental techniques to assess the concrete's performance:

  • Material Preparation: Waste tire rubber was processed into three different particle sizes (10, 20, and 30 mesh). Concrete mixes were prepared with a standard C40 mix ratio, with one group serving as a control (Group A) and others incorporating 20% fine aggregate replacement by mass with the different rubber sizes (Groups B, C, and D).
  • Freeze-Thaw Cycling: Specimens were subjected to accelerated freeze-thaw cycles (up to 125 cycles) using a rapid freezing and melting method at -20°C.
  • Dynamic Impact Testing: The Split-Hopkinson Pressure Bar (SHPB) test device was used to apply dynamic impact loads to the concrete specimens. This device allows for precise measurement of stress, strain, and strain rate under high-speed loading.
  • Microstructural Analysis: Scanning Electron Microscopy (SEM) was utilized to examine the internal microstructure of the concrete before and after freeze-thaw cycles, revealing changes in pore structure and crack formation.
  • Fracture Morphology Analysis: Visual inspection and photographic documentation of the specimens after impact testing were performed to understand the failure modes.

Datasets

Not discussed in the paper. The study relies on experimental data generated from the prepared concrete specimens.

Key Insights and Ideas

  • Rubber as a "Shock Absorber": The addition of rubber particles acts as an energy absorption mechanism during impact. This viscoelastic behavior helps to buffer the applied force, delaying failure and improving the overall integrity of the concrete.
  • Finer Rubber, Better Performance: The study strongly suggests that smaller rubber particle sizes (specifically 30-mesh) lead to superior performance. This is attributed to better particle distribution, more compact structures, and potentially a reduced area of weak bonding between rubber and aggregates.
  • Freeze-Thaw Mitigation: Rubberized concrete, especially with finer particles, shows significantly better resistance to freeze-thaw damage. The internal pores introduced by rubber help to relieve pressure from ice formation, thus reducing internal damage and maintaining higher peak stress after cycling.
  • Strain Rate Correlation: A clear positive correlation was observed between strain rate and dynamic peak stress, and also between strain rate and impact pressure, highlighting the material's response to rapid loading.

Key Results

  • Improved Integrity: Rubberized concrete specimens maintained better integrity after impact, showing less fragmentation and a "loose but not scattered" state compared to ordinary concrete, which exhibited more crushing failure.
  • Enhanced Frost Resistance: After 125 freeze-thaw cycles, the 30-mesh rubber concrete experienced a significantly smaller decrease in peak stress (around 30.7% at 0.6 MPa impact) compared to ordinary concrete (around 52.3%).
  • Impact Resistance: The addition of rubber, particularly 30-mesh, significantly improved impact resistance. The peak stress of rubberized concrete was generally higher than that of ordinary concrete after freeze-thaw cycles, and the 30-mesh group consistently outperformed the 10-mesh and 20-mesh groups.
  • Microstructural Changes: SEM analysis revealed that rubber incorporation led to denser concrete with fewer large holes but more small pores, which are crucial for mitigating freeze-thaw damage.

Limitations and Future Work

  • Limited Freeze-Thaw Cycles: While 125 cycles were tested, exploring a wider range of freeze-thaw cycles could provide a more comprehensive understanding of long-term durability.
  • Specific Impact Pressures: The study focused on three specific impact pressures. Investigating a broader spectrum of impact loads could further refine the understanding of the material's behavior.
  • Mix Design Variations: The study used a fixed rubber replacement ratio (20% of fine aggregate mass). Exploring different replacement ratios and combinations of rubber particle sizes could yield optimized mix designs.
  • Future Work Suggestions: The authors suggest that this research can provide new ideas for the engineering application of rubber concrete, particularly in cold regions. Further investigation into the long-term performance and cost-effectiveness of these rubberized concrete formulations would be beneficial for widespread adoption.

Summary updated

Abstract

To improve the long-term performance of concrete engineering in high-altitude areas, waste tire rubber was added to a concrete mix, and freeze–thaw and impact tests were conducted. The effects of waste tire rubber with different particle sizes (10, 20, 30 mesh) and freeze–thaw cycles (0, 25, 50, 75, 100, 125) on the dynamic mechanical properties of concrete materials were studied. The stress–strain curves, peak stress, and fracture morphology of the specimens were analyzed. The microstructure changes of the specimens were also analyzed using scanning electron microscopy (SEM). The results showed the following: (1) Both macroscopic and microscopic analysis results showed that the internal damage of rubber concrete specimens was smaller after freeze–thawing, and the integrity was better after impact, maintaining a loose but not scattered state. The addition of waste tire rubber significantly improved the material’s impact resistance to a certain extent. (2) As the impact pressure increased, the strain rate of the specimens increased linearly, and the dynamic peak stress was linearly positively correlated with the strain rate. (3) After 125 freeze–thaw cycles, the peak stress of the specimens with 30-mesh added rubber decreased significantly less than that of ordinary concrete under 0.3, 0.45, and 0.6 MPa impact pressure. The dynamic peak stress was higher than that of specimens with 10-mesh and 20-mesh added rubber, and the addition of 30-mesh rubber significantly improved the frost resistance and impact resistance of concrete materials. This study can provide new ideas for the engineering application of rubber concrete.
BibTeX
@article{huang2024experimental,
  author = {Xiaowen Huang and Tengsheng Yue and Jun Zhang and Jinsong Zhang},
  title = {{Experimental Research on the Impact Resistance Mechanical Properties and Damage Mechanism of Rubberized Concrete under Freeze–Thaw Cycling}},
  journal = {Journal of Composites Science},
  year = {2024},
  doi = {10.3390/jcs8030087},
}
Figure