TL;DR
This study experimentally investigates how the geometry of vertical fissures (width, length, and number) in rock specimens affects their mechanical behavior under cyclic loading. The findings reveal that the number of fissures has the most significant impact, influencing peak stress, energy dissipation, and damage evolution, which is crucial for understanding and mitigating rock burst risks in underground engineering.
What Problem Does This Paper Address?
Rock bursts are a major hazard in mining and tunneling, often triggered by the failure of layered rock structures with pre-existing cracks. While the general principles of rock deformation and failure under cyclic loading are understood, the specific influence of the geometry of these "layer-crack" structures on their mechanical behavior and failure mechanisms remains poorly understood. This knowledge gap hinders the development of effective rock burst mitigation strategies. This paper aims to systematically investigate how variations in fissure width, length, and number impact the strength, deformation, energy evolution, and damage accumulation in layer-crack rock specimens under cyclic uniaxial compression.
Methods
The researchers prepared layer-crack sandstone specimens with controlled vertical fissure geometries. They then subjected these specimens to cyclic uniaxial compression tests. The testing involved applying cyclic loads up to a certain stress level and then unloading, repeating this process multiple times before loading to failure. Key parameters measured and analyzed included:
- Stress-strain curves: To understand the overall deformation and failure characteristics.
- Peak stress and peak strain: To quantify the strength and deformation capacity.
- Elastic modulus: To assess the stiffness of the material during loading and unloading.
- Energy evolution: Quantifying input energy, elastic energy, and dissipated energy using the areas under the stress-strain curves.
- Damage variable: Calculated based on dissipated energy to track the accumulation of internal damage.
- Acoustic Emission (AE) events: To monitor micro-fracturing activity during the tests.
The study systematically varied fissure width (1.0-2.5 mm), fissure length (20-80 mm), and the number of fissures (0-3) to isolate the effects of each geometric parameter.
Datasets
Not discussed in the paper. The study relies on experimental data generated from prepared rock specimens.
Key Insights and Ideas
- Cyclic loading strengthens specimens: Counterintuitively, cyclic loading generally increased the peak stress of layer-crack specimens compared to monotonic loading. This is attributed to crack closure and improved compatible deformation during the initial low-load cycles.
- Fissure number is king: The number of fissures emerged as the most influential geometric parameter, significantly impacting peak stress, elastic modulus, and damage accumulation. More fissures generally led to lower strength and higher damage.
- Energy dissipation is key to failure: As specimens approached failure, the rate of dissipated energy density increased dramatically, indicating that this energy absorption is a primary driver of failure.
- Damage evolution is concave: The damage variable showed a consistent concave increasing trend with the number of cycles, meaning damage accumulates more rapidly in later stages.
- AE events signal impending failure: Acoustic emission events remained low until shortly before specimen failure, at which point they surged, mirroring the damage evolution pattern.
Key Results
- Peak stress increase: Cyclic loading increased peak stress by approximately 7.82%–17.35% compared to monotonic loading.
- Fissure geometry influence (strongest to weakest): Number > Length > Width.
- Fissure width effect: Slightly influenced mechanical properties; wider fissures did not significantly weaken the specimens.
- Fissure length effect: Shorter fissures (20-40 mm) weakened specimens, while longer fissures (60-80 mm) strengthened them under cyclic loading.
- Fissure number effect: Increasing the number of fissures from 0 to 3 decreased peak stress by 31.04% and significantly reduced elastic modulus.
- Energy evolution: Input, elastic, and dissipated energy densities all increased with the number of cycles. Dissipated energy showed the most accelerated increase near failure.
- Damage evolution: Damage increased non-linearly with cycles. For a given number of cycles, damage increased with more fissures but decreased with longer fissures.
- AE events: Occurred just before failure, with cumulative AE events decreasing as the number of fissures increased, suggesting different failure modes (splitting vs. shear).
Limitations and Future Work
The study acknowledges that the influence of fissure geometry on AE evolution characteristics is "slight." While the paper provides valuable insights into layer-crack specimens, it focuses on sandstone. Future work could explore these phenomena in other rock types, such as coal, which are also prone to rock bursts. Further investigation into the specific failure mechanisms associated with different fissure geometries and their correlation with AE event characteristics could also enhance our understanding and predictive capabilities for rock burst mitigation. The authors also suggest that these results can provide basic data for further research on rock bursts related to layer-crack structure failures.
Summary updated