Enhanced Photocatalytic and Antibacterial Performance of ZnO Nanoparticles Prepared by an Efficient Thermolysis Method

Md. Abu Hanif, Insup Lee, Jeasmin Akter, Md. Islam, Zahid Ali, Kamal Prasad Sapkota, Jae Ryang HahnCatalysts 2019 · DOI

TL;DR

This paper presents a simple, eco-friendly thermal method for synthesizing zinc oxide nanoparticles (ZnO-NPs) that exhibit superior photocatalytic and antibacterial properties. These ZnO-NPs efficiently degrade methylene blue dye and inhibit the growth of E. coli at low concentrations, outperforming previously reported ZnO-NPs.

What Problem Does This Paper Address?

The paper addresses the need for efficient and environmentally friendly methods to produce zinc oxide nanoparticles (ZnO-NPs) with enhanced photocatalytic and antibacterial activities. Traditional synthesis methods often involve harsh chemicals, expensive catalysts, or complex procedures. ZnO-NPs are valuable for applications like organic pollutant degradation and antimicrobial agents, but their effectiveness can be limited by synthesis methods that result in impurities, poor crystallinity, or unfavorable morphology. The authors aim to develop a straightforward, cost-effective, and greener approach to synthesize ZnO-NPs that overcome these limitations.

Methods

The researchers employed a modified thermal method, specifically thermolysis, to synthesize ZnO-NPs. This involved heating zinc acetate dihydrate (ZAD) in a sealed stainless-steel chamber at 550 °C for 10 hours, followed by slow cooling. This method is highlighted for its simplicity and the use of only one chemical precursor.

Characterization techniques included:

  • X-ray Diffraction (XRD): To determine the crystal structure, phase purity, and crystallinity of the synthesized ZnO-NPs.
  • Field-Emission Scanning Electron Microscopy (FE-SEM) and Transmission Electron Microscopy (TEM): To analyze the morphology, particle size, and aggregation of the ZnO-NPs. High-resolution TEM (HR-TEM) was used to examine the lattice structure.
  • Energy Dispersive X-ray Spectroscopy (EDS): To confirm the elemental composition and purity of the synthesized materials.
  • UV-Vis Absorption Spectroscopy: To investigate the optical properties, specifically the bandgap and light absorption characteristics, which are crucial for photocatalysis.
  • Thermogravimetry/Differential Thermal Analysis (TG/DTA): To assess the thermal decomposition of the precursor (ZAD) and the thermal stability of the resulting ZnO phase.

Photocatalytic activity was evaluated by monitoring the degradation of methylene blue (MB) dye under UV irradiation. Antibacterial activity was assessed against Escherichia coli using a microbroth dilution method to determine the Minimum Inhibitory Concentration (MIC).

Datasets

Not discussed in the paper. The study relies on experimental synthesis and characterization, with no mention of pre-existing datasets for training or evaluation.

Key Insights and Ideas

  • Simplicity and Eco-friendliness: The modified thermal method using only zinc acetate dihydrate is a significant advantage, offering a greener and more straightforward alternative to complex chemical syntheses.
  • Morphology Matters: The synthesized ZnO-NPs exhibit a nearly spherical, aggregated shape. This morphology, combined with their small size and high crystallinity, is proposed to enhance both photocatalytic and antibacterial activities due to increased surface area and light-scattering effects.
  • Redshifted Absorption: The UV-Vis spectra show a redshift in the absorption peak, indicating enhanced light absorption, which is critical for efficient photocatalysis. This redshift is attributed to the nanoparticle size and morphology.
  • Potent Antimicrobial Action: The ZnO-NPs demonstrate significant antibacterial activity against E. coli at remarkably low concentrations (MIC of 30–50 µg/mL), surpassing the effectiveness of many previously reported ZnO-NPs.

Key Results

  • Photocatalytic Performance: The synthesized ZnO-NPs achieved an excellent methylene blue degradation efficiency of 99.7% within 80 minutes of UV irradiation. Approximately 50% of the dye was degraded within the first 20 minutes.
  • Antibacterial Activity: The Minimum Inhibitory Concentration (MIC) of the synthesized ZnO-NPs against E. coli was determined to be 30–50 µg/mL. This is a lower concentration than reported for many other ZnO-NP preparations, indicating superior antibacterial efficacy.
  • Material Properties: XRD confirmed the hexagonal wurtzite structure with high crystallinity. FE-SEM and TEM revealed smooth, nearly spherical, aggregated nanoparticles with an average size of approximately 119 nm. UV-Vis spectroscopy indicated a bandgap of 3.23 eV, slightly lower than pure ZnO, contributing to enhanced photocatalysis.

Limitations and Future Work

  • Mechanism Clarity: While the paper proposes a photocatalytic mechanism involving *OH and O2⁻ radicals, the precise interaction mechanism of ZnO-NPs with biomolecules and microorganisms remains an area for further investigation.
  • Environmental Impact and Human Safety: The authors acknowledge that zinc oxide can be harmful to the environment and toxic to aquatic organisms. While small amounts are used therapeutically, the long-term human safety of these specific synthesized ZnO-NPs is not fully established and warrants further study.
  • Broader Applications: The study focused on MB degradation and E. coli inhibition. Future work could explore the photocatalytic and antibacterial performance of these ZnO-NPs against a wider range of organic pollutants and microbial strains.
  • Optimization: While the method is efficient, further optimization of synthesis parameters could potentially lead to even finer control over particle size, morphology, and thus, enhanced performance.

Summary updated

Abstract

ZnO nanoparticles (ZnO-NPs) were synthesized by a straightforward modified thermal method using only one chemical: zinc acetate dihydrate. The process is environmentally safer than other methods because it does not involve other chemicals or a catalyst, acid, or base source. X-ray diffraction analysis indicated that the ZnO-NPs crystallize in the hexagonal wurtzite structure. The UV–vis absorption spectra revealed a marked redshift, which is critical for enhanced photocatalytic activity. We used methylene blue for photocatalytic activity tests and found an excellent degradation percentage (99.7%) within a short time (80 min). The antibacterial activity of the synthesized ZnO-NPs was tested against Escherichia coli at different concentrations of ZnO-NPs. The analysis revealed that the minimum inhibitory concentration (MIC) of the ZnO-NPs against E. coli was 30–50 μg/mL. Our ZnO-NPs were found to be more effective than previously reported ZnO-NPs synthesized via other methods.
BibTeX
@inproceedings{hanif2019enhanced,
  author = {Md. Abu Hanif and Insup Lee and Jeasmin Akter and Md. Islam and Zahid Ali and Kamal Prasad Sapkota and Jae Ryang Hahn},
  title = {{Enhanced Photocatalytic and Antibacterial Performance of ZnO Nanoparticles Prepared by an Efficient Thermolysis Method}},
  booktitle = {Catalysts},
  year = {2019},
  doi = {10.3390/catal9070608},
}
Figure