Efficient Methylcyclohexane Dehydrogenation Catalysis by Al2O3-Supported Pt-Fe Alloy Cluster Catalysts

Rong Xu, Hossein Akhoundzadeh, Lizhen Liu, Yuan Sheng, Mudi Wu, Xin Zhao, Zheng Wang, Chi Cheng Chong, Huey Lim Voon, Yan LiuResearch Square 2024 · DOI

TL;DR

Researchers have developed a high-performance Pt-Fe alloy catalyst supported on alumina ($\text{Al}_2\text{O}_3$) that significantly improves the efficiency of hydrogen release from methylcyclohexane (MCH). By using a unique sodium ferric EDTA precursor, the team created subnanometer "raft-like" clusters that achieve record-breaking hydrogen evolution rates and exceptional long-term stability by suppressing the carbon buildup (coking) that typically kills platinum catalysts.

What Problem Does This Paper Address?

Hydrogen is a clean energy frontrunner, but storing and transporting it as a gas is difficult and dangerous. Liquid Organic Hydrogen Carriers (LOHCs), like the methylcyclohexane/toluene (MCH/TOL) system, offer a solution: they store hydrogen in a stable liquid form that can be handled using existing gasoline infrastructure.

The "bottleneck" is the dehydrogenation step—getting the hydrogen back out. Standard platinum-on-alumina ($\text{Pt}/\text{Al}_2\text{O}_3$) catalysts are the industry go-to, but they suffer from two major flaws:

  1. Deactivation: Large platinum clusters tend to get "choked" by carbon deposits (coking) during the reaction.
  2. Low Selectivity: Platinum often triggers side reactions, like cracking or isomerization, producing unwanted byproducts instead of pure toluene.

Methods

The authors synthesized a series of bimetallic catalysts using a novel approach. Instead of standard metal salts (like nitrates or chlorides) which often aggregate into large, inefficient chunks, they utilized a sodium ferric ethylenediaminetetraacetate (Na-Fe-EDTA) precursor.

Key techniques used to verify their results included:

  • STEM & EDS Mapping: To visualize the subnanometer "raft-like" structures and confirm that Fe and Na were perfectly dispersed alongside Pt.
  • CO-DRIFT & XPS: To probe the electronic environment of the Pt atoms, revealing how the addition of Fe changes how molecules bind to the surface.
  • XAS (XANES/EXAFS): To confirm the actual formation of a Pt-Fe alloy bond and measure the coordination environment at the atomic level.
  • Operando Testing: Measuring catalytic performance under harsh, real-world reaction conditions ($370^\circ\text{C}$, high flow rates).

Datasets

As an experimental catalysis paper, the "datasets" consist of performance metrics across various catalyst formulations:

  • Primary Catalyst: $\text{Pt-Fe1.2-Na0.6}/\text{Al}_2\text{O}_3$ (the optimized version).
  • Control Groups: Pure $\text{Pt}/\text{Al}_2\text{O}_3$, catalysts with Fe but no Na, catalysts with Na but no Fe, and catalysts made using standard iron nitrate ($\text{Fe}(\text{NO}_3)_3$) precursors.
  • Performance Benchmarks: Comparison against a wide range of recently reported Pt-based catalysts in literature (summarized in the paper's Table S5).

Key Insights and Ideas

  • The "Dilution" Effect: Atomically dispersed Iron (Fe) acts as a spacer. By diluting the Platinum (Pt) ensembles, it prevents the formation of large Pt "islands" where coke precursors usually take root.
  • Electronic Modulation: Fe transfers electrons to Pt. This "electron-rich" Pt has a lower affinity for the reaction products, allowing toluene to detach more easily before it can decompose into carbon soot.
  • The Role of Sodium (Na): While Fe handles the Pt clusters, Na plays a crucial defensive role by neutralizing the acidic sites on the $\text{Al}_2\text{O}_3$ support. These acidic sites are the primary culprits behind the formation of "five-membered ring" side products.
  • Precursor Synergy: The EDTA ligand provides steric hindrance during the manufacturing process, effectively "locking" the metal atoms in place and preventing them from clumping together during high-temperature treatment.

Key Results

  • Record Activity: The optimized catalyst achieved a hydrogen evolution rate of $2729 \text{ mmol}\cdot\text{gPt}^{-1}\cdot\text{min}^{-1}$, significantly higher than previously reported benchmarks.
  • Exceptional Stability: While standard Pt catalysts often degrade within hours, this alloy maintained its conversion efficiency for over 160 hours with only a minor $2.1\%$ drop.
  • High Selectivity: The system achieved $>99.9\%$ selectivity for toluene, with methane and other side products reduced to negligible levels ($<0.01\%$).
  • Coke Resistance: Post-reaction analysis showed a dramatic reduction in carbon formation compared to monometallic Pt catalysts.

Limitations and Future Work

The authors acknowledge that while the Na-Fe-EDTA precursor is highly effective, the exact mechanism of how Fe dispersion levels influence the Pt-Fe interaction requires deeper study. They also note that while 160 hours is excellent for a laboratory setting, industrial-scale LOHC systems will eventually require catalysts that can survive for thousands of hours. Future research will likely focus on the long-term "regeneration" cycles of these alloy clusters and testing them with more complex LOHC molecules.

Summary updated

Abstract

<title>Abstract</title> Methylcyclohexane (MCH) has emerged as one of the most promising liquid organic hydrogen carriers. The conventional Pt/Al<sub>2</sub>O<sub>3</sub> catalyst for MCH dehydrogenation faces issues of deactivation and low selectivity due to the suboptimal characteristics of Pt. To address these challenges, we developed a Pt-Fe alloy catalyst by modifying Al<sub>2</sub>O<sub>3</sub>-supported subnanometer Pt clusters with a sodium ferric ethylenediaminetetraacetate precursor. Spectroscopic and microscopic data reveal that the atomically dispersed Fe dilutes Pt ensemble and modulates its electronic properties through the formation of subnanometer raft-like Pt-Fe alloy, leading to enhanced catalytic stability. Furthermore, Na species suppress the formation of five-membered ring side products, thereby improving the overall selectivity. Remarkably, the Pt-Fe1.2-Na0.6/Al<sub>2</sub>O<sub>3</sub> catalyst demonstrates exceptional performance, including high selectivity and stability, and a high hydrogen evolution rate of 2729 mmol·gPt<sup>− 1</sup>·min<sup>− 1</sup>. This superior performance can be attributed to the profound modulation of electronic and geometric properties of Pt within the bimetallic structure, which mitigates coke formation.
BibTeX
@inproceedings{xu2024efficient,
  author = {Rong Xu and Hossein Akhoundzadeh and Lizhen Liu and Yuan Sheng and Mudi Wu and Xin Zhao and Zheng Wang and Chi Cheng Chong and Huey Lim Voon and Yan Liu},
  title = {{Efficient Methylcyclohexane Dehydrogenation Catalysis by Al2O3-Supported Pt-Fe Alloy Cluster Catalysts}},
  booktitle = {Research Square},
  year = {2024},
  doi = {10.21203/rs.3.rs-3878260/v1},
}
Figure