Effect of carbon substitution on the magnetic properties and crystalline phases of melt-spun<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">Nd</mml:mi></mml:mrow><mml:mrow><mml:mn>4</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math><mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">Fe</mml:mi></mml:mrow><mml:mrow><mml:mn>77.5</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math><mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">B</mml:mi></mml:mrow><mml:mrow><mml:mn>18.5</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math>alloys
Lists
Only you see this
Abstract
The magnetic properties and crystallized phases of melt-spun ${\mathrm{Nd}}_{4}$${\mathrm{Fe}}_{77.5}$${\mathrm{B}}_{18.5\mathrm{\ensuremath{-}}\mathit{x}}$${\mathrm{C}}_{\mathit{x}}$ (x=0, 4, 6, 8, and 10) alloys have been investigated by means of zero-field spin-echo nuclear magnetic resonance (NMR), x-ray diffraction, and magnetization measurements. The results show that the Curie temperatures of amorphous alloys have a small dependence on carbon concentration, the saturation magnetization of amorphous alloys and the average magnetic moment per Fe atom are found to have a small increase, as x increases from x=0 to x=10, and, the crystallization temperatures of amorphous alloys decrease with increasing carbon concentration. The amorphous alloys are magnetically soft; their coercive fields are less than 10 Oe. When the ribbons are annealed over the crystallization temperature, the coercivity increases rapidly and reaches a maximum value at the annealing temperature of about 670 \ifmmode^\circ\else\textdegree\fi{}C, then decreases monotonically. Previous studies demonstrated that ${\mathrm{Nd}}_{4}$${\mathrm{Fe}}_{77.5}$${\mathrm{B}}_{18.5}$ alloys annealed at 670 \ifmmode^\circ\else\textdegree\fi{}C for a short time consisted only of body-centered-tetragonal ${\mathrm{Fe}}_{3}$B (bct ${\mathrm{Fe}}_{3}$B) and a few percent of \ensuremath{\alpha}-Fe. After a short anneal at 670 \ifmmode^\circ\else\textdegree\fi{}C, the coercivity of crystallized alloys decreases with increasing carbon content, with a simultaneous development of an orthorhombic ${\mathrm{Fe}}_{3}$B(o-${\mathrm{Fe}}_{3}$B) phase. Furthermore, the NMR study demonstrates that o-${\mathrm{Fe}}_{3}$B has softer magnetic properties than bct ${\mathrm{Fe}}_{3}$B. It can be concluded that the addition of carbon in ${\mathrm{Nd}}_{4}$${\mathrm{Fe}}_{77.5}$${\mathrm{B}}_{18.5}$ alloy favors the transformation from bct ${\mathrm{Fe}}_{3}$B to o-${\mathrm{Fe}}_{3}$(B,C) and the decrease of coercivity is due to the presence of o-${\mathrm{Fe}}_{3}$(B,C).
BibTeX
@inproceedings{cheng1995effect,
author = {Zhao‐Hua Cheng and Bao-gen Shen and Fangwei Wang and Lei Cao and ZHAO JIAN-GAO and Wen-shan Zhan and Ming-Xi Mao and Ji‐Jun Sun and Fashen Li and Yide Zhang},
title = {{Effect of carbon substitution on the magnetic properties and crystalline phases of melt-spun<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">Nd</mml:mi></mml:mrow><mml:mrow><mml:mn>4</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math><mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">Fe</mml:mi></mml:mrow><mml:mrow><mml:mn>77.5</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math><mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" display="inline"><mml:mrow><mml:msub><mml:mrow><mml:mi mathvariant="normal">B</mml:mi></mml:mrow><mml:mrow><mml:mn>18.5</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math>alloys}},
booktitle = {Physical},
year = {1995},
doi = {10.1103/physrevb.51.12433},
}Loading related content...