Direct Reduction of Zinc Sulfide Concentrate with Coal and Calcium Carbonate

Chuanfu Zhang, Iwazo Asakura, Osamu OgawaJournal of the Mining and Metallurgical Institute of Japan 1988 · DOI

Abstract

In a former report the authors have proposed a new method to prepare strong briquettes for the vertical retort zinc smelting process by mixing zinc sulfide concentrate with pulverized coal and calcium oxidefollowed by preheating, briquetting, and coking. In the present study, calcium carbonate has been substituted for calcium oxide because the latter quickly reacts with moisture in the ambient atmosphere and causes the briquette to collapse in a day or two. The coked briquette with calcium carbonate is as strong as the one with calcium oxide, does not collapse after being left in the laboratory for weeks, and is faster for zinc sulfide to be reduced. Fixation of sulfur during the reduction of zinc sulfide is excellent and substantially all the sulfur is fixed in the form of CaS. Although the specific resistance at room temperature, 29.2Ωcm, of the coked briquette in this study in abtut six times as large as that of the former one with calcium oxide, it easily decreased to about 23Ωcm when heated to about 100°, which suggests the possibility of feeding the briquette into not only a vertical retortbut also an electrothermic furnace without additional coke.
BibTeX
@article{zhang1988direct,
  author = {Chuanfu Zhang and Iwazo Asakura and Osamu Ogawa},
  title = {{Direct Reduction of Zinc Sulfide Concentrate with Coal and Calcium Carbonate}},
  journal = {Journal of the Mining and Metallurgical Institute of Japan},
  year = {1988},
  doi = {10.2473/shigentosozai1953.104.1209\_837},
}

Loading related content...

Figure