Comparative Analysis of the Recovery of Cu2+ and Au from Washing Solution of Pyrite Concentrate Slag by Two Processes

Kun Zhu, Lei Qi, Libo ZhangMinerals 2024 · DOI

TL;DR

This paper presents two novel processes for recovering valuable copper (Cu²⁺) and gold (Au) from the washing solution of pyrite concentrate slag, a significant industrial waste. Both iron powder replacement and neutralization precipitation followed by micropore filtration proved effective, with iron powder replacement achieving slightly higher recovery rates, while neutralization precipitation offered better economic benefits due to lower costs.

What Problem Does This Paper Address?

Pyrite concentrate slag, a byproduct of sulfuric acid production, is generated in massive quantities globally. This slag contains valuable metals like copper and gold, but its washing solution is often treated using traditional methods that are environmentally damaging and inefficient, leading to resource waste. Current methods can also cause operational issues like pipeline blockage. The authors aim to address this by developing and comparing two advanced, comprehensive recovery schemes for Cu²⁺ and Au from this specific washing solution, which contains approximately 437 mg/L of Cu²⁺ and 0.13 mg/L of Au.

Methods

The study compares two distinct processes for recovering Cu²⁺ and Au:

  1. Iron Powder Replacement-Micropore Filtration: This method leverages the principle of electrochemical displacement. Iron powder, being more reactive than copper, reduces Cu²⁺ ions in the solution to metallic copper, which precipitates as sponge-like particles. Simultaneously, granular gold, which doesn't react directly with iron, is "co-precipitated" with the copper particles. The resulting mixture is then filtered using microporous filter cloths (with pore sizes < 1 µm) to separate the solid products. The study systematically investigated the optimal conditions for this process, including pH, iron powder dosage, and replacement time.
  2. Neutralization Precipitation-Micropore Filtration: In this approach, Cu²⁺ ions are precipitated as copper hydroxide (Cu(OH)₂) by adjusting the solution's pH using sodium hydroxide. Similar to the first method, granular gold is then co-precipitated with the copper hydroxide due to mutual adsorption. The precipitate is subsequently filtered using microporous filter cloths (< 1 µm pore size). The research focused on determining the optimal pH for precipitation and the effectiveness of different filter pore sizes.

Both processes utilize atomic absorption spectroscopy for quantitative analysis of Cu²⁺ and Au concentrations and calculate recovery rates.

Datasets

The study utilized a washing solution sample sourced from a gold smelter's pyrite concentrate slag in Yunnan Province, China. The composition of this solution was analyzed and is presented in Tables 1 and 2, detailing element concentrations and the particle size distribution of gold. No new benchmark datasets were introduced; the research focused on optimizing recovery from a real-world industrial waste stream.

Key Insights and Ideas

  • Co-precipitation is Key: Both methods rely on the "co-precipitation" of gold with the primary metal (copper) due to mutual adsorption. This is crucial for recovering the fine gold particles.
  • Iron's Reactivity Advantage: Iron powder's higher standard redox potential compared to copper makes it an effective reducing agent for Cu²⁺, leading to efficient metallic copper recovery.
  • Micropore Filtration is Essential: The use of filter cloths with very small pore sizes (< 1 µm) is critical for effectively capturing the fine precipitated gold and copper particles in both processes.
  • pH Sensitivity: The recovery efficiency for both copper and gold is significantly influenced by pH. For iron powder replacement, a slightly acidic pH (around 3.0) was optimal, while for neutralization precipitation, a near-neutral pH (around 6.5) was preferred.
  • Economic Trade-offs: While iron powder replacement yielded slightly higher recovery rates, the neutralization precipitation process demonstrated superior economic benefits due to lower material costs (NaOH vs. iron powder).

Key Results

  • Iron Powder Replacement:
    • Optimal conditions: pH 3.0, 6 g/L iron powder, 3.0 h replacement time, < 1 µm filter pore size.
  • Recovery rates: Cu²⁺ at 98.13%, Au at 95.83%.
  • Neutralization Precipitation:
    • Optimal conditions: pH 6.5, < 1 µm filter pore size.
  • Recovery rates: Cu²⁺ at 97.35%, Au at 93.54%.
  • Economic Analysis: The neutralization precipitation process resulted in a higher annual profit (65.78 million CNY) compared to iron powder replacement (55.55 million CNY), primarily due to lower production costs.

Limitations and Future Work

  • Limitations:
    • The study focused on a specific washing solution composition from one location. The applicability to other sources with different impurity profiles might vary.
  • While economic benefits are highlighted, a full lifecycle assessment or detailed cost-benefit analysis beyond material consumption and sales revenue could provide a more comprehensive picture.
  • Future Work:
    • The authors suggest that the neutralization precipitation-micropore filtration process, with its lower material consumption, lower cost, and obvious economic benefits, is expected to be widely adopted in similar gold enterprises. Further research could explore scaling up this process and optimizing it for continuous operation.
  • Investigating the potential for recovering other valuable elements present in smaller quantities in the washing solution could also be a future direction.

Summary updated

Abstract

A large amount of pyrite concentrate slag washing solution is produced in China every year, and this contains valuable components such as Cu2+ and Au. The traditional treatment method not only pollutes the environment but also wastes metal resources. For the washing solution containing Cu2+ 437 mg/L and Au 0.13 mg/L, two new processes comprehensive recovery schemes were developed and compared in this paper, namely iron powder replacement pore filtration and neutralization precipitation pore filtration. When the iron powder replacement pore filtration process was adopted, Cu2+ and Au were mainly comprehensively recovered in the form of a mixture of sponge copper and particulate gold. The test results showed that the replacement optimal conditions involved a pH of 3.0, iron powder dosage of 6 g/L, and replacement time of 3.0 h. After replacement, the filter cloth with below 1 μm pore size was used for filtration. The recovery rate of Cu2+ in the washing solution was 98.13 and the total recovery rate of Au was 95.83%. Otherwise, when the neutralization precipitation pore filtration process was adopted, Cu2+ and Au were mainly comprehensively recovered in the form of a mixture of copper hydroxide and particulate gold. The test results showed that sodium hydroxide was used as the precipitant and the optimum neutralization pH value was 6.5. After precipitation, the filter cloth with a below 1 μm pore size was used for filtration. The recovery rate of Cu2+ in the washing solution was 97.35% and the total recovery rate of Au was 93.54%. The economic benefit estimation of the two processes showed that the neutralization precipitation pore filtration process had the advantages of low material consumption, low cost and high economic benefit.
BibTeX
@inproceedings{zhu2024comparative,
  author = {Kun Zhu and Lei Qi and Libo Zhang},
  title = {{Comparative Analysis of the Recovery of Cu2+ and Au from Washing Solution of Pyrite Concentrate Slag by Two Processes}},
  booktitle = {Minerals},
  year = {2024},
  doi = {10.3390/min14090921},
}
Figure