Abstract
Steep-wavefront impulse overvoltages, including fast-front overvoltage (FFO) with wavefront times of 0.1–20 $\mu s$, are generated during disconnector switch operations in gas-insulated equipment (GIE), posing a threat to insulation integrity. This study investigates the breakdown characteristics of the $SF_6$ alternative $C_4F_7N/CO_2$ mixtures under FFO. The influence of wavefront time, gas pressure, and voltage polarity was examined in both slightly non-uniform and extremely non-uniform electric fields. Results indicate that $C_4F_7N/CO_2$ mixtures exhibit insulation properties similar to $SF_6$, with a 9% $C_4F_7N$ mixture reaching approximately 78% to 90% of $SF_6$ strength. The 50% breakdown voltage ($U_{50\%}$) follows a "U-curve" relative to wavefront time in slightly non-uniform fields and an "N-curve" relative to pressure in extremely non-uniform fields under positive polarity.
Introduction
For decades, the electrical power industry has relied on sulfur hexafluoride ($SF_6$) for high-voltage insulation due to its exceptional dielectric strength. However, $SF_6$ is a potent greenhouse gas with a global warming potential (GWP) approximately 23,500 times that of $CO_2$. Consequently, identifying eco-friendly alternatives is a priority for sustainable power grid development.
Heptaperfluoroisobutyronitrile ($C_4F_7N$) has emerged as a leading candidate. While its performance under steady-state AC and DC conditions is well-documented, its behavior under transient stresses like Fast-Front Overvoltages (FFO) is critical for real-world application. FFO are rapid voltage spikes (0.1–20 $\mu s$) occurring during switching operations in gas-insulated equipment. This paper evaluates how $C_4F_7N/CO_2$ mixtures withstand these steep surges.
Experimental Methodology
The experimental investigation compared a 9% $C_4F_7N$ / 91% $CO_2$ mixture against pure $SF_6$ across a range of pressures (0.1 to 0.7 MPa).
The test setup featured a 600 kV impulse voltage generator and a specialized test chamber. To simulate various field conditions, two electrode geometries were employed: sphere-plane (slightly non-uniform) and needle-plane (extremely non-uniform). The "up-and-down" method was used to determine the 50% breakdown voltage ($U_{50\%}$), and COMSOL Multiphysics was utilized for electric field modeling.
Impulse Waveform Characteristics
The study focused on the "steepness" of the wavefront. Five distinct wavefront times ($T_f$) were generated to observe the gas's response to varying rates of voltage rise.
As shown in the figure above, the wavefront time significantly influences the breakdown process, as it dictates the time available for electron avalanche formation and space charge accumulation.
Results and Discussion
The U-Curve Phenomenon
In slightly non-uniform fields, the $U_{50\%}$ vs. $T_f$ relationship follows a U-shaped curve. At extremely short wavefront times, the voltage required for breakdown is high because the rapid rise doesn't allow sufficient time for the initial electron avalanche to bridge the gap. Conversely, at longer wavefront times, the voltage rises again due to the accumulation of space charges (ions) that shield the electrodes and homogenize the electric field.
The N-Curve and Corona Stabilization
In extremely non-uniform fields under positive polarity, the breakdown voltage vs. pressure graph exhibits an "N-curve." This is attributed to corona stabilization: as pressure increases, a corona discharge forms around the needle tip, creating a protective ion cloud that effectively increases the breakdown voltage. However, at higher pressures, this corona layer is compressed, reducing its protective effect and causing a temporary dip in breakdown strength before it rises again due to increased gas density.
Polarity and Pressure Effects
The mixture is highly sensitive to polarity in non-uniform fields. Under negative impulses, the $U_{50\%}$ tends to saturate with increasing pressure, lacking the complex N-curve behavior seen in positive impulses. In slightly non-uniform fields, the breakdown voltage increases linearly with pressure, reaching approximately 78% to 90% of $SF_6$ performance. The authors also derived empirical parameters for the standard breakdown equation $U_{50\%} = a(Pd)^n f^m$, allowing for predictive modeling.
Conclusion
The 9% $C_4F_7N/CO_2$ mixture demonstrates insulation performance comparable to $SF_6$ under FFO conditions. The identification of characteristic U-curves and N-curves provides essential data for the insulation coordination of next-generation, eco-friendly gas-insulated equipment. Future work should address the liquefaction limits in cold climates and the long-term chemical stability of the mixture under repeated discharge.
Summary updated