Abstract
The authors report the deposition of 4.5-nm-thick cobalt (II) oxide on SiO2/Si(001) and MgO(001) substrates at 180–270 °C by atomic layer deposition using bis(N-tert-butyl-N′-ethylpropionamidinato) cobalt (II) and water as coreactants. The resulting CoO film is smooth and carbon-free. CoO can be reduced to Co metal using hydrogen or deuterium gas at 400–500 °C in a vacuum furnace, but the high temperature processing causes dewetting, leading to discontinuous Co metal islands rather than continuous films. Two low temperature (∼200 °C) reduction methods are reported: deuterium atom reduction and the use of an O-scavenging Al metal film. The low temperature methods can suppress dewetting to a large extent, and the resulting metallic cobalt film is smooth and continuous.
BibTeX
@article{zhang2018atomic,
author = {Zizhuo Zhang and Himamshu C. Nallan and Brennan M. Coffey and Thong Q. Ngo and Tanmoy Pramanik and S. Banerjee and John G. Ekerdt},
title = {{Atomic layer deposition of cobalt oxide on oxide substrates and low temperature reduction to form ultrathin cobalt metal films}},
journal = {Journal of Vacuum Science \& Technology A Vacuum Surfaces and Films},
year = {2018},
doi = {10.1116/1.5063669},
}Ask Althea to put this paper to the test.
Loading related content...