NeurIPS 2026Coming to NeurIPS?Explore papers, orals & directions

Atmospheric Pressure Chemical Vapor Deposition of Copper Thin Films: I . Horizontal Hot Wall Reactor

Wing-cheong Lai, Yibo Xie, G. L. GriffinJournal of The Electrochemical Society 1991

Abstract

We have studied the reaction kinetics of Cu chemical vapor deposition (CVD) by H2 reduction of Cu(hfa)2 in a horizontal flow, atmospheric pressure, hot-wall CVD reactor. Using glass substrates, we can routinely deposit films at temperatures as low as 523 K and growth rates of 200 A/min, with resistivities between 2–3 μΩ-cm. The reactor is operated at integral conversions of Cu(hfa)2, and the reaction kinetics are determined by analyzing the axial thickness profiles of the deposited films obtained under a series of different operating conditions (e.p. reactant composition, substrate temperature, and carrier gas flow rate). The steady-state growth rate exhibits saturation kinetics with respect to Cu(hfa)2 concentration, positive reaction order with respect to H2, and negative reaction order with respect to H(hfa). We propose a mechanism based on dissociative adsorption of Cu(hfa)2 at vacant surface sites, followed by H-atom assisted desorption of H(hfa) ligdnds as the rate limiting step in the overall reaction. The resulting rate expression is combined with a reactor model based on a one-dimensional Cu(hfa)2 species conservation equation, and the calculated thickness profiles are compared with observed results to obtain estimates of the kinetic parameters. © 1991, The Electrochemical Society, Inc. All rights reserved.
BibTeX
@article{lai1991atmospheric,
  author = {Wing-cheong Lai and Yibo Xie and G. L. Griffin},
  title = {{Atmospheric Pressure Chemical Vapor Deposition of Copper Thin Films: I . Horizontal Hot Wall Reactor}},
  journal = {Journal of The Electrochemical Society},
  year = {1991},
  doi = {10.1149/1.2085441},
}

Loading related content...

Figure