Abstract
The sintering of limonite ore is a recent cost-effective method of iron production. In this study, the influences of sinter binary basicity and calc-flux type on the quantity, strength, and type of sintering bonding phases, as well as on sinter quality under high limonite ratios, were investigated by an experiment based on the characteristics of ore blends. Production of sinters demonstrates that, under high limonite ratios, sinter quality can be improved by increasing the binary basicity of sinters, the ratio of quicklime, and the height of the sintering bed.
Introduction
As high-grade iron ore becomes scarcer and more expensive, steelmakers are turning to cheaper alternatives like limonite. However, limonite is a difficult material for the sintering process—the step where iron ore fines are fused into larger, porous lumps for blast furnace use. Due to its high crystal water content and large particle size, limonite often exhibits "strong assimilability," leading to a weak liquid bonding phase during heating. This typically results in sinters that crumble easily (low drum index) and poor production yields. This study identifies the specific chemical and process adjustments—basicity, flux types, and bed height—required to transform low-quality limonite blends into high-performing sinter.
Experimental Methodology
The researchers conducted laboratory experiments and sintering pot tests using an ore blend containing 45% limonite (61.13% TFe, 4.39% LOI). The study focused on two primary variables:
- Binary Basicity ($CaO/SiO_2$): Tested across a range from 1.8 to 2.1.
- Calc-Flux Type: Compared traditional limestone ($CaCO_3$) against more reactive quicklime ($CaO$).
To evaluate performance, the "flowing area method" was used to measure bonding phase fluidity, and mineralogical analyses identified the crystalline structures formed, specifically focusing on calcium ferrite, the primary contributor to sinter strength.
Analysis of Bonding Phase Characteristics
A critical finding of the study is the superior performance of quicklime over limestone in generating the necessary bonding phase. Quicklime's higher reactivity and structural density allow it to produce a significantly larger quantity of liquid phase at lower temperatures.
As illustrated in the experimental data, bonding phase fluidity increases with both temperature and binary basicity. Notably, quicklime blends achieve higher fluidity at 1220°C than limestone blends do at 1240°C, facilitating better granulation and stronger sinter structures at lower thermal inputs.
Key Insights and Results
- Optimal Basicity: Sinter strength follows an "inverse V" relationship with basicity, peaking at a binary basicity of 2.0. Beyond this point, the sinter becomes excessively porous and brittle.
- The Role of Calcium Ferrite: Increasing the volume of calcium ferrite not only strengthens the sinter but also improves its "reducibility," or how easily it releases oxygen in the blast furnace.
- Productivity Gains: Increasing binary basicity from 1.8 to 2.1 improved sintering productivity by up to 11%. Using 6.0 wt% quicklime at a basicity of 2.1 resulted in the highest yield (82.21%) and the best drum index (65.62%).
- Basicity Segregation: Mineralogical analysis revealed that because large iron particles (>1mm) do not react fully with the flux, the "local" basicity in bonding areas is significantly higher (calculated at ~4.43 to 5.22) than the target "bulk" basicity.
Conclusion and Future Outlook
Optimizing the sintering of high-limonite blends requires a targeted approach to chemistry and flux selection. By utilizing quicklime and maintaining a binary basicity of approximately 2.0, producers can achieve high-quality sinter with improved fuel efficiency. Future research should investigate the maximum threshold for limonite ratios before quality degrades regardless of optimization, as well as the environmental impacts of shifting to high-limonite, high-quicklime blends.