A Mechanical Investigation on the Phase Transition Behavior of La0.7Ca0.3MnO3—δ Ceramics
Abstract
The characteristics of the phase transition of polycrystalline La0.7Ca0.3MnO3—δ (LCMO) was investigated by using the vibrating reed method. The internal friction (Q—1) of the sample shows two peaks: P1 and P2. The first internal friction peak, P1, appears in heating up and cooling down indicative of a paramagnetic to ferromagnetic phase transition with a considerable resonant frequency drop at the transition point. The second broader internal friction peak, P2, appears only in heating up and its corresponding frequency (f) exibits a maximum. Additionally, the P1 temperature was found to be linked with a thermal absorption peak and a variation of the magnetization and the electric resistance.
BibTeX
@inproceedings{chen1999mechanical,
author = {X. B. Chen and Jianming Zhu and G. H. Hwang and C.M. Fu and H. M. Duh and C. H. Lin and Weicheng Gao and X. Y. Mao and Y. N. Wang},
title = {{A Mechanical Investigation on the Phase Transition Behavior of La0.7Ca0.3MnO3—δ Ceramics}},
booktitle = {Physica Status Solidi (a)},
year = {1999},
doi = {10.1002/(sici)1521-396x(199906)173:2<451::aid-pssa451>3.0.co;2-u},
}Ask Althea to put this paper to the test.
Loading related content...